Thermally activated regeneration of spent LiFePO4 with a nitrogen and phosphorus co-doped carbon layer for lithium extraction from salt-lake brine.
Yang Bao, Yuhao Pan, Yufeng Da, Hongshan Wang, Luwei Miao, Ke Li, Xurui An, Yongzheng Fu,
College of Architecture and Environment, Sichuan University, Chengdu, 610065, China. · Facultad de Ciencias y Centro de Investigación en Ciencias de La Salud y Biomedicina (CICSAB), Universidad Autónoma de San Luis Potosí, Av. Sierra Leona 550, San Luis Potosi, S. L. P., 78210, Mexico.
Key points
From the paper's conclusion- Redirecting regenerated S-LFP to lithium extraction therefore connects spent-battery recycling with salt-lake lithium recovery, with Mg co-uptake and counter-electrode durability identified as the main remaining constraints.
Abstract
Spent LiFePO4 (S-LFP) cathodes and Mg-rich salt-lake brines are conventionally handled by separate industries. Here, S-LFP powder was converted into a lithium-selective electrode for hybrid capacitive deionization (HCDI) through a two-stage thermal treatment with LiOH·H2O and discarded cooked egg yolk, which couples lithium replenishment with the growth of an N,P-co-doped carbon shell. In the optimized material, R-LFP@CNP20, the Li/Fe molar ratio recovered from 0.87 to 1.05, the heterosite FePO4 reflections disappeared, and a locally 2-4 nm carbon coating formed. In 1 M LiCl, R-LFP@CNP20 delivered 157.4 mAh g-1 at 1 C and 121.8 mAh g-1 at 10 C, showed the lowest charge-transfer resistance (1.66 Ω) and retained 92.9% of its capacity after 120 cycles at 10 C. In HCDI, it captured 6.46 mg g-1 Li+ from an 8.18 mg L⁻¹ feed with the lowest adsorption-step energy consumption of the series. It retained 70.3% of its adsorption capacity after 100 cycles and released 52.8% less Fe than S-LFP, and anode-replacement tests indicated a substantial counter-electrode contribution to full-cell decay. In Qinghai brine with a Mg/Li molar ratio of 9.9, the Li/Mg separation factor reached 7.42, and the Li fraction of the adsorbed cations increased from 9.0 to 41.2 mol%. Redirecting regenerated S-LFP to lithium extraction therefore connects spent-battery recycling with salt-lake lithium recovery, with Mg co-uptake and counter-electrode durability identified as the main remaining constraints.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Direct Repair of the Crystal Structure and Coating Surface of Spent LiFePO4 Materials Enables Superfast Li-Ion MigrationNano-Micro Letters · 2026
- CO2-assisted selective lithium extraction and closed-loop regeneration of spent NCM cathodes toward cleaner battery recycling.RSC advances · 2026
- Direct Regeneration of Spent LiFePO 4 Cathodes by Liquid‐Phase‐Mediated ReconstructionChemSusChem · 2026
- Scalable Hydrometallurgical Process for LFP Battery Recycling with Selective Lithium Extraction and Iron StabilizationProcesses · 2026
- Defect-to-Phase Transduction and Interface Reconstruction Enable Regeneration of Spent LiFePO4 Cathodes.Nano-micro letters · 2026
- Microenvironment‐Regulated Interfacial Reconstruction Enables High‐Performance Direct Regeneration of Spent LiFePO 4 CathodesAdvanced Functional Materials · 2026