In vitro evaluation of sliding contact wear performance in direct resin-based composites with varying inorganic filler loadings.
F Cinelli, G T Rocca, E Di Bella, M Mekki, R Michelotto Tempesta, N Scotti, J G Leprince, L Giachetti,
Dental Materials and Restorative Dentistry, Department of Experimental and Clinical Medicine, Unit of Dentistry, University of Florence, Florence, Italy. · Division of Cariology and Endodontology, School of Dentistry, University of Geneva, Geneva, Switzerland.
Key points
From the paper's conclusion- Under the tested conditions, wear performance differed significantly among the six commercial RBCs, and higher inorganic mass fractions were associated with lower volume loss. The independent contribution of filler content could not be isolated from other compositional and microstructural differences among the commercial formulations.
Abstract
OBJECTIVES: To evaluate the two-body wear performance and behavior of commercially available direct resin-based composites (RBCs) spanning a broad range of inorganic filler loadings. METHODS: 144 disc-shaped specimens (5 mm × 2 mm) were prepared from six commercial RBCs selected according to manufacturer-reported filler loading (vol%): ELS (E), 49%; Tetric EvoCeram (T), 53-55%; Filtek Z250 (Z), 60%; Inspiro (I), 65%; Grandio (G), 71.4%; and Clearfil Majesty Posterior (M), 82%. Specimens underwent two-body wear testing in a dual-axis chewing simulator (CS-4.8) against stainless-steel antagonists (5°C/55°C, 49 N, 1.8 Hz) for 150,000, 300,000, or 600,000 cycles (n = 8/group). Volume loss was measured by confocal optical profilometry; digital microscopy and scanning electron microscopy provided qualitative assessment. Thermogravimetric analysis (TGA) estimated the inorganic filler mass fraction (wt%). Data were analyzed using two-way ANOVA and linear regression (α = 0.05). RESULTS: Volume loss increased with cycle count. Two-way ANOVA revealed significant effects of composite type and cycle count and a significant interaction (all p < 0.001). At 600,000 cycles, mean (SD) volume loss ranged from 2.896 (0.292) mm3 for Grandio to 6.502 (0.948) mm3 for ELS. Higher inorganic mass fractions were associated with lower volume loss at all cycle counts (p < 0.001; R2 = 0.234-0.655), with regression slopes differing across loading intervals (p < 0.001). Microscopy revealed subsurface microcracking; no micro-pitting was observed. CONCLUSION: Under the tested conditions, wear performance differed significantly among the six commercial RBCs, and higher inorganic mass fractions were associated with lower volume loss. The independent contribution of filler content could not be isolated from other compositional and microstructural differences among the commercial formulations.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Wear performance of different bulk-fill class II resin composite restorations: 3-year clinical evaluationScientific Reports · 2026
- Intraoral Scanner Evaluation of Cyclic Wear in Heated Versus Injectable Composites for Indirect Restoration.European journal of dentistry · 2026
- Wear resistance of three direct resin composites in artificial Saliva at varying pH levelsFrontiers in Dental Medicine · 2025
- Evaluation of the Effect of Different Light-Curing Protocols on the Microhardness of Contemporary Bulk-Fill Resin CompositesPolymers · 2025
- Strain Distribution at the Composite-Tooth Interface: An In Vitro Study Using Digital Image Correlation and Linear Mixed-Effects Models.Clinical and experimental dental research · 2026
- Effect of toothbrushing mode and brushing load on the wear of anterior tooth-shaped restorative composites.Odontology · 2026