OCT for Evaluation of a Universal Adhesive in a Three-Year Clinical Trial.
Rainer Haak, Matthias Häfer, Ellen Schulz-Kornas, Tobias Meißner, Hartmut Schneider
Department of Cariology, Endodontology and Periodontology, University of Leipzig, Liebigstraße 12, 04103 Leipzig, Germany. Electronic address: rainer.haak@medizin.uni-leipzig.de. · Department of Cariology, Endodontology and Periodontology, University of Leipzig, Liebigstraße 12, 04103 Leipzig, Germany. Electronic address: matthias.haefer@medizin.uni-leipzig.de.
Key points
From the paper's conclusion- Clinical assessments and OCT-based analyses were consistent. In terms of bond failure, however, the groups already differed upon restoration placement, with reproducible substrate-specific differences becoming apparent.
Abstract
OBJECTIVES: In parallel with the 36-month clinical evaluation of a universal adhesive, tooth-composite bond failure was assessed by tomography. METHODS: In 55 patients, three non-carious cervical lesions (NCCLs) each were restored with FiltekTM Supreme XTE (3M) using the universal adhesive Scotchbond™ Universal Adhesive (SBU, 3M) in the self-etch (SE) or selective enamel-etch (SEE) mode or by OptiBond™ FL (OFL, Kerr, reference, randomization). Immediately after restoration placement (T0) and in parallel with the clinical assessments (FDI criteria) at 6, 12, 24, and 36 months (M), the restorations were imaged by optical coherence tomography (OCT) to quantify interfacial adhesive defects (ADs; 14 days, clinical only). Cumulative failure rates (CFRs) and means of ADs were statistically analyzed. RESULTS: From six to 36M, CFRs were lower in the SBU groups vs. OFL (pi ≤ 0.004). Compared to SBU-SE or OFL, SBU-SEE resulted in reduced marginal staining (≥ 12M; pi: 0.002 - 0.727) and increased marginal adaptation (≥ 12M; pi: 0.001 - 0.629). Increased ADs appeared on the enamel with SBU-SE vs. SBU-SEE and OFL (T0 - 36M; pi ≤ 0.001/0.048) and with OFL vs. SBU-SEE (≥ 6M; pi ≤ 0.025). At dentin/cement less defects appeared using SBU-SEE vs. SBU-SE (≥ 6M) or OFL (≥ T0, pi ≤ 0.0115), and fewer in the SBU-SE vs. OFL group (≥ T0, pi ≤ 0.001). Before restoration loss, the adhesive defects on the dentin/cement were increased (pi ≤ 0.05). CONCLUSIONS: Clinical assessments and OCT-based analyses were consistent. In terms of bond failure, however, the groups already differed upon restoration placement, with reproducible substrate-specific differences becoming apparent. CLINICAL SIGNIFICANCE: The universal adhesive Scotchbond™ Universal Adhesive in SEE mode performed most favorably. Interfacial adhesive defects detectable by OCT reliably predict the performance of a restoration system. #DRKS00011084, http://www.drks.de/DRKS00011084, 30.09.2016.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- How laser etching affects the clinical performance of a "no-wait" universal adhesive: 36-month results.Clinical oral investigations · 2026
- The Effect of Different Types of Adhesive Systems on Marginal Integrity of Class II Resin Composite Restoration.The journal of adhesive dentistry · 2026
- Determination of marginal permeability of restorations in the cervical region using a universal adhesive system: a randomized controlled open-label laboratory studyRussian Journal of Dentistry · 2026
- Comparative assessment of the resin-dentin interface using three different universal adhesives: An ex vivo studyJournal of Conservative Dentistry and Endodontics · 2026
- Radiographic appearance of proximal resin composite restorations bonded with a radiopaque or radiolucent universal adhesive: a randomized clinical trial.BDJ open · 2026
- Microtensile bond strength and dentin–adhesive interface of universal adhesives before and after artificial aging: an in vitro studyScientific Reports · 2026