Trade-off between ion transport and interfacial stability in all-solid-state cathodes with high active material fraction.
Zhe Li, Bowen Liu, Jing Wu, Miao Xu, Kai Yang, Dongyan Wang, Yi Wang, Chunhao Yuan,
Jiangsu Key Laboratory of Electrochemical Energy-Storage Technologies, College of Materials Science and Technology, Nanjing University of Aeronautics and Astronautics, No. 29 Yudao Street, Nanjing 210016, China. · Center for Microscopy and Analysis, College of Materials Science and Technology, Nanjing University of Aeronautics and Astronautics, Nanjing 211106, PR China.
Key points
From the paper's conclusion- Single-crystal LiNi0.94Co0.03Mn0.03O2 (NCM94) and Li3InCl6 (LIC) were used as a model system to study the trade-off between ion transport and interfacial stability in all-solid-state cathodes.
- At CAM fractions of 80-85 wt%, the high-energy ball milling of nanosized LIC forms a continuous coating layer on NCM94, improving rate capability and cycling stability. However, at 90 wt%, interfacial damage leads to rapid impedance growth and performance decay.
- Introducing a lithium niobate (LiNbO3) interlayer mitigates interfacial degradation, highlighting the trade-off between ion transport and interfacial deterioration for halide-based composite cathodes.
Abstract
Halide solid-state electrolytes are promising catholyte candidates for high energy density all-solid-state batteries (ASSBs). However, for halide-based composite cathodes, achieving high cathode active material (CAM) fractions while maintaining efficient ionic transport and interfacial stability remains a critical challenge. Here, we employ single-crystal LiNi0.94Co0.03Mn0.03O2 (NCM94) and Li3InCl6 (LIC) as a model system to elucidate the trade-off effects between ion transport connectivity and interfacial degradation. High-energy ball milling disperses nanosized LIC and forms a continuous coating layer on NCM94, constructing a three-dimensional Li+ transport network that significantly improves rate capability and cycling stability at CAM fractions of 80-85 wt%. At a CAM fraction of 90 wt%, however, mechanically induced interfacial damage offsets transport gains, leading to rapid impedance growth and performance decay. Introducing a lithium niobate (LiNbO3) interlayer mitigates this interfacial degradation. This work highlights the trade-off between ion transport and interfacial deterioration, providing guidance for designing halide-based composite cathodes.
Read the paper
Discussion · 1
Science Skim's AI key points, plus readers' public thoughts
- Single-crystal LiNi0.94Co0.03Mn0.03O2 (NCM94) and Li3InCl6 (LIC) were used as a model system to study the trade-off between ion transport and interfacial stability in all-solid-state cathodes.
- At CAM fractions of 80-85 wt%, the high-energy ball milling of nanosized LIC forms a continuous coating layer on NCM94, improving rate capability and cycling stability. However, at 90 wt%, interfacial damage leads to rapid impedance growth and performance decay.
- Introducing a lithium niobate (LiNbO3) interlayer mitigates interfacial degradation, highlighting the trade-off between ion transport and interfacial deterioration for halide-based composite cathodes.
Readers' thoughts
No reader thoughts yet.
Related papers
- A paradigm shift in all-solid-state lithium batteries: halide cathode materials streamlined for multi-electron reactions.National science review · 2026
- Halide-Based Mixed Ionic-Electronic Conductors Deliver High-Rate and Long-Life All-Solid-State Lithium Batteries.Advanced materials (Deerfield Beach, Fla.) · 2026
- Tailoring Local Anion Chemistry Affinity Enables Stable Halide-Sulfide Interfaces and Fast Ion Transport in Dual-Electrolyte all-Solid-State Batteries.Angewandte Chemie (International ed. in English) · 2026
- Interphase-Adaptive Chloride Solid Electrolyte Enables High-Performance All-Solid-State Lithium Batteries.ACS nano · 2026
- Outward Charge-Enriched Boundaries Stabilize Halide-Sulfide Solid-Electrolyte Interfaces.Inorganic chemistry · 2026
- Amorphous Halide Cathodes Enable 75C All-Solid-State Lithium Batteries.Journal of the American Chemical Society · 2026