Journal of the American Chemical Society

Amorphous Halide Cathodes Enable 75C All-Solid-State Lithium Batteries.

Yuhao Duan, Feng Wan, Fiaz Hussain, Jiuwei Lei, Zihan Song, Paul R Shearing, Wei Xia, Zhuangjun Fan,

Division of Energy Storage, Dalian National Laboratory for Clean Energy, Dalian Institute of Chemical Physics, Chinese Academy of Sciences, Dalian116023, China. · Eastern Institute for Advanced Study, Eastern Institute of Technology, Ningbo315201, China.

Key points

From the paper's conclusion
  • The study reveals that minimizing grain-boundary transport barriers in halide cathode active materials (CAMs) unlocks ultrafast ion-transport.
  • Amorphous LiVCl4 delivers a capacity of 74.3 mAh g-1 at 5 mA cm-2, compared with 10.2 mAh g-1 for the crystalline counterpart, and operates across a wide temperature range from -30 to 60 °C.
  • Coupled with amorphous LiTaOCl4, the ASSLB achieves 102.1 mAh g-1 at 20 mA cm-2 (∼75C) and retains 82.3% capacity after 16,000 cycles.

Abstract

Power delivery in all-solid-state lithium batteries (ASSLBs) is often pursued by maximizing the bulk ionic conductivity of cathode active materials (CAMs), while grain-boundary (GB) ion-transport barriers caused by lattice mismatch remain a major kinetic bottleneck. Here, we reveal that minimizing GB transport barriers, rather than simply enhancing intrinsic conductivity, unlocks ultrafast ion-transport in halide CAMs. Amorphization converts crystalline LiVCl4 into a conformal amorphous phase that preserves short-range V-Cl coordination while minimizing long-range ion-transport tortuosity. Despite lower bulk Li+ conductivity, amorphous LiVCl4 dramatically reduces GB-associated interfacial resistance and enables a catholyte-free cathode (CAM content: 90 wt %) to deliver a capacity of 74.3 mAh g-1 at 5 mA cm-2, compared with 10.2 mAh g-1 for the crystalline counterpart. Meanwhile, the ASSLB further operates across a wide temperature range from -30 to 60 °C and achieves 84.2% capacity utilization at an ultrahigh A-LiVCl4 areal loading of 53.4 mg cm-2. Coupled with amorphous LiTaOCl4, the ASSLB achieves 102.1 mAh g-1 at 20 mA cm-2 (∼75C) and retains 82.3% capacity after 16,000 cycles. These results establish amorphization-enabled conformal interfaces as a new paradigm for ultrahigh-power ASSLBs.

Read the paper

Discussion · 1

Science Skim's AI key points, plus readers' public thoughts

Science SkimAI key points
Pinned
  • The study reveals that minimizing grain-boundary transport barriers in halide cathode active materials (CAMs) unlocks ultrafast ion-transport.
  • Amorphous LiVCl4 delivers a capacity of 74.3 mAh g-1 at 5 mA cm-2, compared with 10.2 mAh g-1 for the crystalline counterpart, and operates across a wide temperature range from -30 to 60 °C.
  • Coupled with amorphous LiTaOCl4, the ASSLB achieves 102.1 mAh g-1 at 20 mA cm-2 (∼75C) and retains 82.3% capacity after 16,000 cycles.

Readers' thoughts

No reader thoughts yet.

Related papers