From the paper's conclusion
  • The Ca(OH)₂/cation-exchange route produced a predominantly amorphous calcium-containing cyclotriphosphate material in which no sodium signal was detected by EDS. This material provided greater protection against initial enamel erosive softening and mineral loss than NaCTP and 0.24% NaF.

Abstract

OBJECTIVES: This study synthesized calcium-containing cyclotriphosphate materials from sodium cyclotriphosphate (NaCTP) using calcium hydroxide [Ca(OH)₂], calcium chloride (CaCl₂), or calcium nitrate [Ca(NO₃)₂], designated Ca(OH)₂-CTP, CaCl₂-CTP, and Ca(NO₃)₂-CTP, respectively, and evaluated their effects on initial enamel erosion. The powders were characterized by scanning electron microscopy (SEM), energy-dispersive X-ray spectroscopy (EDS), Fourier-transform infrared spectroscopy (FTIR), and X-ray diffraction (XRD). DESIGN: Bovine enamel blocks (n = 10/group) were allocated to placebo; 0.24% sodium fluoride (NaF); or 0.5% and 1% NaCTP, Ca(OH)₂-CTP, CaCl₂-CTP, or Ca(NO₃)₂-CTP groups. After toothpaste treatment (2 min), blocks underwent four erosive cycles (1 min; pH 3.5). Surface hardness was assessed after treatment and each challenge. Micro-computed tomography measured mineral concentration and lesion depth. Data were analyzed by analysis of variance and Tukey's test (p < 0.05). RESULTS: CaCl₂-CTP and Ca(NO₃)₂-CTP showed partial sodium replacement by EDS and crystalline structures by XRD. For Ca(OH)₂-CTP, no sodium signal was detected by EDS; the material retained characteristic cyclotriphosphate bands by FTIR and exhibited a predominantly amorphous structure by XRD. NaF and NaCTP showed similar mineral loss (p ≥ 0.086). Ca(OH)₂-CTP produced significantly lower hardness loss and mineral depletion than all other groups (p < 0.001) and reduced lesion depth by approximately 50% relative to NaCTP and NaF. CONCLUSIONS: The Ca(OH)₂/cation-exchange route produced a predominantly amorphous calcium-containing cyclotriphosphate material in which no sodium signal was detected by EDS. This material provided greater protection against initial enamel erosive softening and mineral loss than NaCTP and 0.24% NaF.