Calcium cyclohexaphosphate as a novel bioactive condensed phosphate: synthesis, physicochemical characterization, and protective effects on sound and softened enamel under erosive conditions

Raquel Borges Amancio de Lima, Thamires Priscila Cavazana, Luigi Pedrini Guisso, Leonardo Antônio de Morais, Thayse Yumi Hosida, Juliano Pelim Pessan, João Carlos Silos Moraes, Emerson Rodrigues de Camargo,

Key points

From the paper's conclusion
  • In conclusion, CaCHP was synthesized from NaCHP, and 1% CaCHP provided protection comparable to 0.24% NaF, with persistence depending on enamel condition.

Abstract

Calcium-modified cyclophosphates may enhance protection against enamel demineralization. This study synthesized and characterized calcium cyclohexaphosphate (CaCHP) and evaluated its concentration-dependent protective effect against initial enamel demineralization under erosive conditions in vitro. CaCHP was obtained from sodium cyclohexaphosphate (NaCHP) by ion-exchange resin and characterized by SEM, EDS, XRD, and FTIR. Sound and softened bovine enamel blocks (n = 12/group) were treated with toothpaste slurries prepared in human saliva containing 0.25%, 0.5%, or 1% NaCHP; 0.25%, 0.5%, or 1% CaCHP; 0.24% NaF; or placebo. Blocks underwent four consecutive citric acid challenges (pH 3.5, 1 min), interspersed with surface hardness measurements. Data were analyzed by three-way ANOVA and Tukey tests ( p < 0.05). Enamel surfaces were also examined by SEM/EDS. Characterization confirmed Na replacement by Ca within a cyclic structure and greater crystallinity for CaCHP than NaCHP. All groups showed decreased hardness during acid challenges. However, softened enamel treated with NaF or cyclophosphates showed a smaller decrease in surface hardness than sound enamel ( p < 0.05). Placebo showed the greatest decrease in hardness ( p < 0.05), regardless of initial enamel condition. In sound enamel, 1% CaCHP and 0.24% NaF showed comparable protection through the third acid challenge, but neither differed from placebo after the fourth challenge. In softened enamel, 1% CaCHP remained comparable to 0.24% NaF and significantly more protective than placebo and NaCHP after the fourth challenge ( p < 0.001). In conclusion, CaCHP was synthesized from NaCHP, and 1% CaCHP provided protection comparable to 0.24% NaF, with persistence depending on enamel condition.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers

Calcium cyclohexaphosphate as a novel bioactive condensed phosphate: synthesis, physicochemical characterization, and protective effects on sound and softened enamel under erosive conditions — Science Skim