Archives of Civil and Mechanical Engineering

Near-solidus forming as a potential annealing-free processing route for AISI 316 austenitic stainless steel: experimental validation and environmental assessment

John Damilola Sunday, Alberto Murillo-Marrodán, Phillip Krawec, Eduardo García, Jokin Lozares, Carl Slater

Key points

From the paper's conclusion
  • Near-solidus forming (NSF) is evaluated as a single-step processing route for AISI 316 austenitic stainless steel, combining closed-die forging and microstructural restoration at 1350 $$^\circ \text {C}$$ .

Abstract

Near-solidus forming (NSF) is evaluated as a single-step processing route for AISI 316 austenitic stainless steel, combining closed-die forging and microstructural restoration at 1350 $$^\circ \text {C}$$ . The resulting microstructure and tensile response are compared with an experimentally investigated post-forging annealed condition (NSF + HT, 900 $$^\circ \text {C}$$ for 2 h), while the mechanical properties are additionally evaluated against the minimum requirements reported for annealed AISI 316. Six experimental trials were conducted using a 1200 kN hydraulic press and modelled in Forge NxT 4.1 with a calibrated Hensel–Spittel constitutive model and a JMAK microstructural evolution framework. Peak forging loads of 81–82 t were recorded, and the simulation predicted peak loads within 5–6% of the experimental values. The forged component showed a heterogeneous microstructure, with mean grain sizes of 43.4–58.0 $$\upmu $$ m across six locations. The head exhibited finer grains, partial dynamic recrystallization with necklace morphology toward the exterior and $$\delta $$ -ferrite retained at the centre, whereas the flute exhibited coarser grains and an equiaxed structure consistent with static recrystallization toward the exterior. NSF-forged components achieved a UTS of 542.50 MPa and a fracture strain of 75.72%, both exceeding the minimum specification for annealed AISI 316. The mean UTS differed by 8.92 MPa between the NSF and post-forging annealed conditions, showing similar mean tensile performance in the flute region; the limited sample size does not establish statistical equivalence, and corrosion resistance requires further investigation. A screening life cycle assessment showed that NSF reduced CO $$_2$$ emissions by 65.8% relative to conventional forging plus solution annealing, from 5.06 to 1.73 kg CO $$_2$$ eq kg $$^{-1}$$ , and by 25.7% for NSF followed by post-forging annealing at 900 $$^\circ \text {C}$$ for 2 h (NSF + HT).

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers