Through-Section Characterization of a Large Forged AISI 316 Component: An Industrial Post-Deviation Case Study.

Jude Emele, Aleš Slíva, Mahalingam Nainaragaram Ramasamy, Hasanien Ali Sattar Al Sharif, Jan Dizo

Institute of Transport, Faculty of Mechanical Engineering, VSB Technical University of Ostrava, 17. Listopadu 15, 708 00 Ostrava-Poruba, Czech Republic. · Faculty of Mechanical Engineering, University of Zilina, 17. Univerzitna 8215/1, 010 26 Zilina, Slovakia.

Key points

From the paper's conclusion
  • Thus, pronounced through-section mechanical-property variation occurred without corresponding detectable compositional variation.

Abstract

This industrial case study examines through-section variations in a 341 mm-diameter AISI 316 stainless-steel component following an unintended extended furnace residence during solution annealing. Instead of being rapidly cooled after the prescribed 1.5 h hold, the component remained in the furnace for approximately 22.25 h, including approximately 16 h at or near 1080 °C. Specimens from the nominal surface, half-radius, and central regions were examined using optical microscopy, tensile and Vickers microhardness testing, SEM-EDS, handheld XRF, and ASTM A262 Practice E testing. Reported mean grain size increased from 286 ± 8 µm at the surface to 304 ± 10 µm at the geometric center, although the underlying uncertainty calculations were unavailable for retrospective verification. Mean yield strength was 36.3% lower in the nominal central-region tensile group (r/R = 0.23; 231.3 MPa) than in the near-surface group (r/R = 0.93; 363.3 MPa), while microhardness decreased from 173 to 157 HV0.5. No clear monotonic radial variation was identified in the measured principal alloying elements within the analytical resolution of SEM-EDS and handheld XRF. Post-test visual and SEM examinations revealed no intergranular cracking, grain-boundary separation, or preferential grain-boundary dissolution. Thus, pronounced through-section mechanical-property variation occurred without corresponding detectable compositional variation. Without a conventionally treated control component or direct internal-temperature measurements, the origin of this variation could not be uniquely determined or attributed specifically to the extended furnace residence.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers

Through-Section Characterization of a Large Forged AISI 316 Component: An Industrial Post-Deviation Case Study — Science Skim