Journal of Failure Analysis and Prevention

Investigating Deleterious Phases in a Flange of Superduplex UNS S32750 Superduplex Stainless Steel

R. A. Roco Antunez, S. S. M. Tavares, B. L. da Silva, G. Perez, A. R. Pimenta, J. M. Pardal

Key points

From the paper's conclusion
  • The material suffered an incorrect heat treatment which resulted in a microstructure containing about 12.5% of deleterious phases ( σ and χ ) and only 3.9% of ferrite.

Abstract

This work investigates the severe pitting corrosion of a neck flange in the top side of an offshore platform. The chemical analysis revealed that the material is a stainless steel grade UNS S32750. The material suffered an incorrect heat treatment which resulted in a microstructure containing about 12.5% of deleterious phases ( σ and χ ) and only 3.9% of ferrite. The rapid deterioration of the external surface by pitting motivated the failure analysis and, fortunately, the flange didn’t present brittle fracture in service. The unproper microstructure was characterized by non-destructive (ferritoscope, hardness) and desctructive techniques (XRD, electrochemical anodic polarization, scanning electron microscopy). The corrosion properties could be regenerated by solution treatment at 1100 °C followed by water quenching. Instead, the flange was incorrectly treated at lower soaking temperature and/or slow cooling.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers