科研速览 · Science Skim继续刷下去 · Keep skimming →
◆ International Journal of Electrochemical Science2026-03-24· Materials science

Comparative corrosion performance of super duplex and cast duplex stainless steels in synthetic seawater and 3.5 wt% NaCl

Ángela Viviana Torres Delgado, Mauricio Rincón Ortiz, Ana María Pérez Ceballos

原始摘要(英文原文)· Original abstract
The corrosion behavior of two wrought super duplex stainless steels (SDSS), UNS S32750 and UNS S32760, and a cast duplex stainless steel (DSS), DIN/EN 1.4517, was evaluated in 3.5 wt.% NaCl and ASTM D1141 synthetic seawater at 25, 50, and 70 °C. All materials were assessed in their as-received (as-cast/as-rolled) metallurgical condition, without additional homogenization or solution annealing, to determine their baseline stability limits. Both SDSS grades preserved passivity in synthetic seawater up to 70 °C. In NaCl, S32760 maintained resistance to localized attack at 70 °C, whereas S32750 initiated pitting. The cast alloy showed stable pitting from 50 °C in both electrolytes. Impedance values above 5×10⁵ Ω·cm² at 25 °C decreased with temperature, most significantly for 1.4517, while corrosion-current densities increased three- to five-fold per 25 °C increment but remained below 2 µA·cm² for S32760 in seawater. Pitting potentials for 1.4517 decreased to approximately -50 mV vs. SCE at 70°C in NaCl solution. Performance differences were strongly linked to microstructure and composition: the wrought SDSS displayed finer inter-austenitic spacing (~11–12 µm) and higher PREN (>42), whereas the cast DSS exhibited coarser morphology (~29 µm) and lower PREN (~38). XPS analysis revealed passive films mainly composed of chromium and iron oxides/hydroxides, with chloride exposure promoting Cr 2 O 3 depletion and hydroxide enrichment, correlating with the observed reduction in impedance and passive range. These findings clarify the corrosion-resistance hierarchy of the studied alloys and support material-selection decisions for subsea equipment, desalination systems, and other components operating in aggressive marine environments. • Fine inter-austenitic spacing in wrought SDSS delays localized pit stabilization. • Cast 1.4517 loses passivity above 50°C, while wrought S32760 resists up to 70°C. • Dendritic segregation in the cast alloy drives galvanic micro-cell corrosion. • XPS reveals chloride exposure depletes Cr 2 O 3 and enriches passive film hydroxides.
读原文 · Read the paper ↗

AI 追问PRO

登录后使用 AI 追问

讨论区

登录后参与讨论

相关论文 · Related

Comparative corrosion performance of super duplex and cast duplex stainless steels in synthetic seawater and 3.5 wt% NaCl — 科研速览 Science Skim