Comparison of three occlusal splint material systems manufactured by conventional, subtractive, and additive techniques.
Mariana Farias Rocha, Isabela Vitória de Oliveira Nunes, Natasha Rohrig Assumpção da Motta, Anna Júlia Mendonça Paraíso, May Anny Alves Fraga, Cleocir José Dalmaschio, Rafael Ratto de Moraes, Nathalia Silveira Finck,
School of Dentistry, Federal University of Espírito Santo (UFES), Vitória, ES, Brazil. · Centro Universitário FAESA, Vitória, ES, Brazil.
Key points
From the paper's conclusion- Objectives To compare the thermal–viscoelastic behavior, hygroscopic properties, color stability, and surface morphology of three commercial occlusal splint material systems produced by conventional heat polymerization, CAD/CAM milling, and 3D printing.
Abstract
OBJECTIVES: To compare the thermal-viscoelastic behavior, hygroscopic properties, color stability, and surface morphology of three commercial occlusal splint material systems produced by conventional heat polymerization, CAD/CAM milling, and 3D printing. The null hypothesis was that the three material systems would not differ in thermal-viscoelastic behavior, hygroscopic properties, or color stability. Surface morphology was assessed qualitatively as a complementary outcome. MATERIALS AND METHODS: Heat-polymerized polymethyl methacrylate (HEC), CAD/CAM-milled polymethyl methacrylate (CAD-M), and a 3D-printed photopolymer resin (3DP) were evaluated. Dynamic mechanical analysis was performed to determine glass transition temperature (Tg), tan δ, and thermal heterogeneity (n = 5). Water sorption (WS), solubility (SL), and color change after coffee immersion (ΔE00) were assessed (n = 8). Surface morphology was qualitatively analyzed by atomic force microscopy and scanning electron microscopy. RESULTS: Significant differences were observed among the material systems for thermal and hygroscopic outcomes. CAD-M presented the highest mean Tg (149.58 ± 0.95 °C), the lowest water sorption (18.76 ± 0.56 µg/mm³), the lowest solubility (2.59 ± 0.48 µg/mm³), and a ΔE00 of 2.29 ± 1.20 after 7 days of coffee immersion. Conversely, 3DP showed the lowest Tg (83.18 ± 7.87 °C), highest WS (35.12 ± 0.82 µg/mm³), highest SL (6.16 ± 0.40 µg/mm³), greatest color change, and a more irregular surface morphology. CONCLUSIONS: The three evaluated commercial material systems differed in thermal-viscoelastic behavior, hygroscopic properties, color stability, and surface morphology. Among the specific systems tested, CAD-M showed the most favorable overall laboratory profile. Because each manufacturing approach was represented by a single commercial material with a distinct composition, these differences cannot be attributed exclusively to the manufacturing route. CLINICAL RELEVANCE: Under the in vitro conditions tested, the milled material system showed a higher glass transition temperature and lower water sorption, solubility and coffee-induced discoloration than the 3D-printed system. Whether these laboratory differences translate into differences in the clinical performance of occlusal splints was not assessed in this study.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Analyzing Color, Surface Roughness, and Microhardness on the Unpolished and Polished Surfaces of Occlusal Splint Materials From Conventional and CAD–CAM Fabrication MethodsInternational Journal of Dentistry · 2026
- Biocompatibility of five occlusal splint materials produced by four fabrication methods: an in vitro comparative studyBMC Oral Health · 2026
- Comparative volumetric wear of occlusal splint materials under simulated gastric acid and artificial saliva conditions.BMC oral health · 2026
- Effect of Print Orientation and Post-Curing Duration on the Flexural Strength, Flexural Modulus and Vickers Microhardness of a 3D-Printed Occlusal Splint ResinBioengineering · 2025
- Mechanical Properties of Dental Occlusal Splint Materials After Accelerated Aging in Artificial Saliva: An In Vitro Study.Dentistry journal · 2026
- Effect of Resin Type, Layer Thickness, and Printing Orientation on the Mechanical and Surface Properties of 3D-Printed Occlusal SplintsPolymers · 2026