Mitigation Effect of Internal Hydrogen on External Hydrogen‐Induced Embrittlement in Austenitic Lightweight Steel
Chunxiao Meng, Duoyao Liang, Hong Luo, Haiwei Wu, Lifeng Hou, Yinghui Wei
Key points
From the paper's conclusion- In the presence of external hydrogen, the hydrogen embrittlement of lightweight steel is dominated by grain boundary decohesion based on the hydrogen‐enhanced decohesion mechanism, accompanied by localized plastic deformation around the cracks.
Abstract
The influence of various hydrogen environments on the hydrogen embrittlement behavior of Fe‐30Mn‐8.6Al‐C austenitic lightweight steel was investigated using slow strain rate tensile tests. Under the experimental conditions adopted in this work, external hydrogen induces the most severe hydrogen embrittlement. In the combined internal‐external hydrogen environment, internal hydrogen can mitigate the damage to mechanical properties caused by external hydrogen, showing an approximately 50% relative reduction in hydrogen embrittlement susceptibility compared with the sole external hydrogen condition. Postmortem analysis shows that in the external hydrogen environment, relatively few intergranular cracks are dominant, and these cracks induce hydrogen accumulation and cause significant ductility loss. In contrast, in the combined internal‐external hydrogen environment, numerous intergranular and transgranular cracks initiate and release stress, which slows the propagation of cracks. In the presence of external hydrogen, the hydrogen embrittlement of lightweight steel is dominated by grain boundary decohesion based on the hydrogen‐enhanced decohesion mechanism, accompanied by localized plastic deformation around the cracks.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Hydrogen Embrittlement Resistance of an Austempered Martensite/Bainite Dual-Phase Steel.Materials (Basel, Switzerland) · 2026
- Hydrogen embrittlement in pre-loaded sharply-notched samples of cold-drawn pearlitic steel wires for prestressed concrete structures: a fractographic analysisTheoretical and Applied Fracture Mechanics · 2026
- Study on the transition of hydrogen embrittlement mechanisms in 316L stainless steel under the coupled effects of pre‑strain and TIG weldingMaterials Research Express · 2026
- The effects of hydrogen on the mechanical properties of CoCrFeMnNi high-entropy alloy: Molecular dynamics simulationJournal of Applied Physics · 2026
- Study on Hydrogen Embrittlement Behavior of 316L Austenitic Stainless Steel Based on Digital Image CorrelationJournal of Engineering Materials and Technology · 2026
- Investigation of Welded Joints of Pipelines from an Existing Gas Transmission Network Exposed to Hydrogen—Part II: Some Aspects of the Microstructural Mechanisms of Hydrogen-Assisted Damage and FractureMetals · 2026