Study on the transition of hydrogen embrittlement mechanisms in 316L stainless steel under the coupled effects of pre‑strain and TIG welding
Qian Xu, Mingya Chen, Xingyu Pan, Shuiyong Wang, Wanxiang Zhao, Lin Zhang, Jianfeng Mao
Key points
From the paper's conclusion- These findings clarify the microstructure-dependent transition of HE mechanisms in pre-strained TIG-welded 316L stainless steel and provide guidance for the integrity assessment of welded components in hydrogen service.
Abstract
Hydrogen embrittlement (HE) of TIG-welded 316L austenitic stainless steel is strongly affected by welding-induced microstructural heterogeneity and service-induced plastic pre-strain, but the associated mechanism transition across different regions of the welded joint remains insufficiently understood. In this study, in-situ slow strain rate tensile tests in a 5 MPa hydrogen environment, together with microscopic structure characterizations, were conducted on 316L base metal, weld metal and welded joint specimens with different pre-strain levels. The results show that the weld metal exhibits higher HE susceptibility than the base metal, and HE susceptibility increases with pre-strain in both regions. The welded joint exhibits the most severe degradation, with fracture preferentially occurring near the fusion line and heat-affected zone. In the base metal, pre-strain induces high-density dislocation pile-ups, deformation twins and local α'-martensite formation, while hydrogen promotes localized dislocation activity, indicating that hydrogen-enhanced localized plasticity is the dominant failure mechanism. In the weld metal, the δ-ferrite/austenite phase boundaries, heterogeneous dislocation distribution and strain incompatibility promote local hydrogen accumulation. The observation of slip localization, twin damage and quasi-cleavage features suggests that hydrogen enhanced decohesion may also contribute to failure, together with HELP. These findings clarify the microstructure-dependent transition of HE mechanisms in pre-strained TIG-welded 316L stainless steel and provide guidance for the integrity assessment of welded components in hydrogen service.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Hydrogen Embrittlement Susceptibility of Metallic Welded Joints: A ReviewApplied Sciences · 2026
- Investigation of Welded Joints of Pipelines from an Existing Gas Transmission Network Exposed to Hydrogen—Part II: Some Aspects of the Microstructural Mechanisms of Hydrogen-Assisted Damage and FractureMetals · 2026
- Region-resolved study of hydrogen embrittlement mitigation in CrMoV welds through post-weld heat treatmentInternational Journal of Hydrogen Energy · 2026
- Effect of Pre-Strain on Hydrogen Embrittlement Behavior of Metallic Materials: A Critical Review.Materials (Basel, Switzerland) · 2026
- Study on Hydrogen Embrittlement Behavior of 316L Austenitic Stainless Steel Based on Digital Image CorrelationJournal of Engineering Materials and Technology · 2026
- Hydrogen Embrittlement Resistance of an Austempered Martensite/Bainite Dual-Phase Steel.Materials (Basel, Switzerland) · 2026