Internal Buffering–Interfacial Regulation Synergy Bridges Stability and Kinetics in Microsized Silicon–Carbon Anodes
韦焕明, Xinlu Liu, Enmin Li, Wei Shao, Chenjun Ju, Zhenglong Yang
Tongji University
Key points
From the paper's conclusion- A microspherical Mo/W@Gr–Si anode was developed by integrating a flower-like graphene framework with Mo2N/W2C dual-phase heterostructures.
- The Mo/W@Gr–Si anode exhibits a low Li+ adsorption energy (−2.071 eV) and a reduced diffusion barrier (0.42 eV), delivering a high reversible capacity of 1821 mAh g−1 at 0.1C with an initial coulombic efficiency of 88.12%.
- This work offers a generalizable strategy for bridging interfacial stability and Li+ transport kinetics in high-performance silicon anodes.
Abstract
ABSTRACT Microsized Si/C composite anodes are promising for practical lithium‐ion batteries due to their high tap density and scalability. However, their performance remains constrained by structural degradation and an unstable solid electrolyte interface (SEI), and current strategies fail to address the intrinsic coupling between interfacial chemistry and Li + transport kinetics. Here, a structure‐interface co‐engineered microspherical Mo/W@Gr–Si anode is developed by integrating a flower‐like graphene framework with Mo 2 N/W 2 C dual‐phase heterostructures, enabling simultaneous regulation of Li + adsorption and diffusion. Coupled density functional theory (DFT) calculations and advanced characterizations reveal a mechanism linking interfacial stabilization with Li + transport, where the Mo 2 N/W 2 C heterophase stabilizes an inorganic‐rich SEI and reduces diffusion barriers via electronic structure modulation. Consequently, the Mo/W@Gr–Si anode exhibits a low Li + adsorption energy (−2.071 eV) and a reduced diffusion barrier (0.42 eV), delivering a high reversible capacity of 1821 mAh g − 1 at 0.1C with an initial coulombic efficiency of 88.12%, along with outstanding rate capability and cycling stability. Full cell paired with an NCM523 cathode retains 88.2% capacity after 300 cycles (0.5C), while pouch cells exhibit 84.6% retention after 200 cycles at 2C. This work offers a generalizable strategy for bridging interfacial stability and Li + transport kinetics in high‐performance silicon anodes.
Read the paper
Discussion · 1
Science Skim's AI key points, plus readers' public thoughts
- A microspherical Mo/W@Gr–Si anode was developed by integrating a flower-like graphene framework with Mo2N/W2C dual-phase heterostructures.
- The Mo/W@Gr–Si anode exhibits a low Li+ adsorption energy (−2.071 eV) and a reduced diffusion barrier (0.42 eV), delivering a high reversible capacity of 1821 mAh g−1 at 0.1C with an initial coulombic efficiency of 88.12%.
- This work offers a generalizable strategy for bridging interfacial stability and Li+ transport kinetics in high-performance silicon anodes.
Readers' thoughts
No reader thoughts yet.
Related papers
- Laser-directed covalent Si–N–C bonding at SiOx/3D graphene interface for durable composite anodes in lithium-ion batteryAdvanced Composites and Hybrid Materials · 2025
- A Si‐MoSe₂ Heterostructured Anode with Enhanced Thermal Transport and Electrochemical Performance for Liquid and All‐Solid‐State Lithium‐Ion BatteriesAdvanced Science · 2026
- Silicon Nitride-Enabled Mechanical Reinforcement and Interfacial Catalysis Toward Highly Stable Silicon-Based Anodes.Small (Weinheim an der Bergstrasse, Germany) · 2026
- Covalently Anchored, LiF‐Reinforced Rigid‐Flexible Interphase for Stable Nano‐Si AnodesAdvanced Functional Materials · 2026
- Interfacial Anchoring Effect Enables a Stable and High-Areal-Capacity Silicon/Carbon Composite AnodeACS Sustainable Chemistry & Engineering · 2026
- Metallurgical Interface Engineering Constructing In Situ Li3N-Enriched Interphase: A Bulk-Interface Synergy Strategy Toward Practical Silicon Anodes.Advanced materials (Deerfield Beach, Fla.) · 2026