Covalently Anchored, LiF‐Reinforced Rigid‐Flexible Interphase for Stable Nano‐Si Anodes
Heyang Shen, Benchi Li, Jing Wang, Huiqian Xiong, Hui Li, Yongjin Fang, Yuliang Cao, Q Chen,
Wuhan University
Key points
From the paper's conclusion- Consequently, the nSi@G3‐LiF electrode achieves a remarkably high initial Coulombic efficiency of 91.3%, outstanding rate capability (1754, 1631, and 1301 mAh g −1 at 2, 3, and 5 A g −1 , respectively), and superior long‐term cycling stability, retaining 1465 mAh g −1 after 900 cycles at 2 A g −1 .
Abstract
ABSTRACT Silicon‐based materials are ideal alternatives to conventional graphite anodes in lithium‐ion batteries due to their exceptionally high theoretical capacity. However, the dramatic volume changes of silicon during lithiation/delithiation cause pulverization of active particles and repeated fracture and reformation of the solid electrolyte interphase (SEI) film, severely hindering practical applications. Here, a covalent anchoring in situ crystallization (CAIC) strategy is proposed to construct a multifunctional modification layer composed of triglyme (G3) and nano‐sized LiF on the nano‐silicon surface (denoted as nSi@G3‐LiF). This unique architecture provides multiple synergistic effects: high‐modulus LiF and flexible ether‐chain network buffer volume expansion and dissipate mechanical stress; abundant oxygen coordination sites enable rapid Li + transport; and LiF nanocrystals induce a dense, inorganic‐rich SEI layer that effectively suppresses parasitic reactions. Consequently, the nSi@G3‐LiF electrode achieves a remarkably high initial Coulombic efficiency of 91.3%, outstanding rate capability (1754, 1631, and 1301 mAh g −1 at 2, 3, and 5 A g −1 , respectively), and superior long‐term cycling stability, retaining 1465 mAh g −1 after 900 cycles at 2 A g −1 . This work presents an effective strategy for regulating interfacial mechanics and kinetics through chemical bonding coupled with in situ crystallization reinforcement, offering new insights into interfacial design for silicon‐based anodes.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Interfacial Anchoring Effect Enables a Stable and High-Areal-Capacity Silicon/Carbon Composite AnodeACS Sustainable Chemistry & Engineering · 2026
- Pre‐Constructed Mechano‐Electrochemical Adaptive Solid Electrolyte Interphase to Enhance Li⁺ Diffusion Kinetics and Interface Stability for Chemically Prelithiated SiO AnodesAdvanced Science · 2025
- Dual‐Ion Reconstruction of a LiF/NaF–N‐Rich Hybrid Interphase for Durable Silicon‐Carbon AnodesAdvanced Functional Materials · 2026
- Lithiated PAA‐Coated SiOₓ Anode for Stable and High‐Capacity Lithium‐Ion Batteries: Interfacial Regulation and Volume Expansion SuppressionSmall · 2026
- Additive-Specific SEI Nanostructures on Silicon Anodes Revealed by Cryo-TEM and EELS under Suppressed Bulk AlloyingNano Letters · 2026
- Silicon Nitride-Enabled Mechanical Reinforcement and Interfacial Catalysis Toward Highly Stable Silicon-Based Anodes.Small (Weinheim an der Bergstrasse, Germany) · 2026