Storage-Environment-Dependent Surface Evolution and Electrochemical Degradation of High-Nickel NCM Single-Crystal Cathodes.
Fang Zhang, Xiangyu Chen, Jinquan Bai, Lin Chen, Jitao Yu, Laifa Shen
Jiangsu Key Laboratory of Materials and Technologies for Energy Storage, College of Materials Science and Technology, Nanjing University of Aeronautics and Astronautics, Nanjing, China.
Key points
From the paper's conclusion- In contrast, vacuum and inert-gas atmospheres effectively suppress surface degradation and preserve electrochemical performance.
Abstract
High-nickel ternary single-crystal cathodes are promising for high-energy-density batteries in low-altitude-economy applications owing to their high specific capacity. However, surface residual lithium formation during storage substantially impairs their electrochemical performance. Herein, we investigate the formation mechanisms of surface residual lithium and the associated storage-induced degradation of three single-crystal compositions-NCM613, NCM8866, and NCM9442-under vacuum, humid air, argon, pure CO2, and ultrapure water. Potentiometric titration, x-ray diffraction, x-ray photoelectron spectroscopy, electron microscopy, and electrochemical measurements were combined to elucidate the effects of storage environment and nickel content. The storage atmosphere plays a decisive role in residual-lithium formation. CO2 and humid air markedly promote Li2CO3 formation, while increasing nickel content leads to higher surface residual lithium levels and more pronounced structural degradation. The accumulation of residual lithium is accompanied by near-surface disorder and local layered-to-rock-salt-like reconstruction, together with changes in the surface oxygen and nickel chemical states. These alterations increase Li+ transport impedance and electrode polarization, causing substantial losses in specific capacity, rate capability, and cycling stability. In contrast, vacuum and inert-gas atmospheres effectively suppress surface degradation and preserve electrochemical performance. These findings provide useful guidance for optimizing the storage and handling protocols of high-nickel single-crystal cathodes.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Distinguishing Symptoms From Etiology: A Cascading Degradation Mechanism in Cobalt‐Free Layered CathodesAdvanced Functional Materials · 2026
- Multifunctional Surface Engineering of Ni‐Rich Layered Cathodes for Ultra‐Stable Lithium‐Ion BatteriesChemistry - A European Journal · 2025
- Impact of Oxygen Deficiency on Structural and Electrochemical Properties of Single-Crystalline LiNi0.8Co0.1Mn0.1O2 (NCM 811)ACS Electrochemistry · 2026
- Unveiling the Correlation Between Structural Stability and Electrochemical Characteristics of Single Crystalline Layered Ni‐Rich CathodesSmall · 2025
- WO3-Mediated Conversion of Surface Residual Lithium into a Li2WO4 Protective Layer for Enhanced Air Stability and Electrochemical Performance of Single-Crystal High-Nickel NCM Cathodes.ACS applied materials & interfaces · 2026
- Stress-Coupled Lithium–Ion Transport Deterioration in Ni-Rich NCM Cathodes During Long-Term CyclingEnergy & Fuels · 2026