Distinguishing Symptoms From Etiology: A Cascading Degradation Mechanism in Cobalt‐Free Layered Cathodes

Ye Zhang, Jingyao Yang, Qiusheng Zhang, Yuanyuan Li, Zhiqun Zhou, Hongli Deng, Fangrui Yu, Haitao Huang,

Key points

From the paper's conclusion
  • Herein, this study reveals a “cascading degradation mechanism” that decouples initial disorder from dynamic deterioration, identifying intrinsic oxygen vacancies as the fundamental “etiology” while distinguishing accumulated cation disorder as a “symptom.” Leveraging multi‐scale characterization on model LiNi 0.6 Mn 0.4 O 2 and Density Functional Theory calculations, the results demonstrate that i

Abstract

Cobalt‐free layered cathodes are pivotal for next‐generation lithium‐ion batteries due to their cost‐effectiveness, high energy density, and sustainability. However, the complex interplay between severe structural disorder and intrinsic degradation factors remains elusive, hindering their rational design and practical application. Herein, this study reveals a “cascading degradation mechanism” that decouples initial disorder from dynamic deterioration, identifying intrinsic oxygen vacancies as the fundamental “etiology” while distinguishing accumulated cation disorder as a “symptom.” Leveraging multi‐scale characterization on model LiNi 0.6 Mn 0.4 O 2 and Density Functional Theory calculations, the results demonstrate that intrinsic oxygen vacancies trigger a triple synergistic effect of aggravated lattice distortion, high‐voltage oxygen loss, and accelerated interfacial side reactions, which kinetically facilitates Ni migration, driving irreversible structural degradation. Consequently, this work establishes the Li/Ni disorder accumulation (ΔLi/Ni) in limited cycles as a dynamic indicator for evaluating long‐term stability. Based on this mechanism, the optimized NM‐880 cathode delivers excellent long‐term stability, achieving a 92.37% capacity retention after 400 cycles at 0.5 C. The universality of this indicator is robustly validated in commercial LiNi 0.6 Co 0.2 Mn 0.2 O 2 and LiNi 0.5 Co 0.2 Mn 0.3 O 2 systems. This work signals a paradigm shift in cathode design: moving from optimizing static initial structures to regulating defect‐induced dynamic evolution.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers

Distinguishing Symptoms From Etiology: A Cascading Degradation Mechanism in Cobalt‐Free Layered Cathodes — Science Skim