Synergistic Electrostatic and Mechanical Anchoring at Cathode-Current Collector Junctions for Durable Sodium-Ion Batteries.
Sieun Choi, Myung-Jun Kwak, Min Wook Pin, Joon Ha Chang, Beom Tak Na, Seunghun Park, Wontak Kim, Hyogyeong Jeon,
Department of Battery Convergence Engineering, Kangwon National University, Chuncheon, Republic of Korea. · Advanced Batteries Research Center, Korea Electronics Technology Institute, Saenari-ro, Seongnam, Republic of Korea.
Key points
From the paper's conclusion- The primer-integrated NVP//hard carbon full cells retain 88.7% capacity after 300 cycles, establishing a design framework for reliable cathode-current collector junctions in polyanion-based energy storage systems.
Abstract
Maintaining reliable physical and electrical contact at the cathode-current collector junction remains a critical yet underexplored challenge in sodium-ion batteries (SIBs). In particular, Na3V2(PO4)3 (NVP) cathodes undergo ∼8% volumetric fluctuations during biphasic (de)sodiation, progressively deteriorating the weak van der Waals-governed interface between the polyvinylidene fluoride (PVDF) binder and the aluminum substrate, causing electrical isolation and capacity loss. Despite the widespread industrial use of carbon-primed current collectors, a systematic understanding of their reinforcement mechanisms has been lacking. Herein, we elucidate three synergistic anchoring mechanisms through multi-scale characterization. The carbon primer enhances surface roughness to promote mechanical interlocking, provides a compliant interlayer accommodating cyclic volumetric strain without debonding, and establishes electrostatic bridging between carboxylate functional groups and the fluorinated polymer backbone, as independently confirmed by Fourier transform infrared (FTIR) spectroscopy and X-ray photoelectron spectroscopy (XPS). Control experiments verify that the performance bottleneck lies at the junction rather than in bulk electronic conductivity, while cross-sectional wavelength-dispersive spectroscopy mapping reveals that junction integrity governs sodiation uniformity throughout the electrode thickness. The primer-integrated NVP//hard carbon full cells retain 88.7% capacity after 300 cycles, establishing a design framework for reliable cathode-current collector junctions in polyanion-based energy storage systems.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Mechanistic Insights into Sodium Plating in Hard Carbon Anodes: Electrolyte Design Principles for Practical Medium Voltage Sodium-Ion Full BatteriesACS Energy Letters · 2026
- Thermodynamically Self‐Limiting Presodiation Inducing Homogeneous Inorganic–Organic Polymer‐Skeleton Interphases for Durable Sodium‐Ion BatteriesAdvanced Materials · 2025
- Recent Advances in Presodiation Strategies for Hard Carbon in Sodium-Ion Batteries: Mechanisms of SEI Regulation and Electrochemical Performance.Small (Weinheim an der Bergstrasse, Germany) · 2026
- Anionic Bottom-Up Flux Orchestrated via Hard Carbon Surface Chemistry for Stable Sodium-Ion Batteries.Nano-micro letters · 2026
- Dynamic Li+/Na+-Exchanging Interphase Stabilizes High-Voltage Ni-Rich Cathodes for 557 Wh kg–1 Lithium BatteriesJournal of the American Chemical Society · 2026
- Potential‐Tailored Aryl–Sodium Reagent with Moderate Ionic Binding Strength Enables Precise yet Fast Hard Carbon PresodiationAngewandte Chemie International Edition · 2025