Dynamic Li+/Na+-Exchanging Interphase Stabilizes High-Voltage Ni-Rich Cathodes for 557 Wh kg–1 Lithium Batteries
Wenjie Niu, Ning Zhao, Zizhuo Liang, Pengfei Yu, Zhangquan Peng, Guangmin Zhou, Xiangxin Guo
Key points
From the paper's conclusion- A dynamic interphase is constructed by coating LiNi0.8Co0.1Mn0.1O2 (NCM811) with Na3Zr2Si2PO12 (NZSP) to stabilize high-voltage Ni-rich cathodes.
- The modified cathode retains 80% capacity after 511 cycles at 4.7 V and enables a 4 Ah pouch cell to deliver 557 Wh kg–1 with 80.5% retention over 118 cycles.
- This work demonstrates that a Li+/Na+-exchanging interphase can effectively couple interfacial protection with bulk lattice reinforcement for high-voltage Ni-rich cathodes in high-energy lithium batteries.
Abstract
High-voltage operation of Ni-rich layered cathodes LiNi0.8Co0.1Mn0.1O2 (NCM811) accelerates electrolyte decomposition at the surface and destabilizes the bulk lattice with oxygen loss. Conventional strategies for regulating the cathode–electrolyte interphase (CEI) commonly suppress persistent parasitic reactions at Ni-rich cathode surfaces, but increase interfacial polarization and offer limited protection against structural degradation in the bulk. Here, a dynamic interphase is constructed by coating NCM811 with a Na+-based solid-electrolyte Na3Zr2Si2PO12 (NZSP). During cycling, Li+/Na+ exchange transforms the NZSP layer into a fast Li+ conducting interphase LixNa3–xZr2Si2PO12 (L-NZSP), while the Na+ ions are incorporated into the NCM811 lattice. The L-NZSP suppresses parasitic reactions at high charging voltages. Meanwhile, the incorporated Na+ ions provide pillar-like support for the layered framework, stabilizing the oxygen lattice and mitigating chemo-mechanical degradation. Consequently, the modified cathode retains 80% capacity after 511 cycles at 4.7 V and enables a 4 Ah pouch cell to deliver 557 Wh kg–1 with 80.5% retention over 118 cycles. This work demonstrates Li+/Na+-exchanging interphase as an effective strategy to couple interfacial protection with bulk lattice reinforcement for high-voltage Ni-rich cathodes in high-energy lithium batteries.
Read the paper
Discussion · 1
Science Skim's AI key points, plus readers' public thoughts
- A dynamic interphase is constructed by coating LiNi0.8Co0.1Mn0.1O2 (NCM811) with Na3Zr2Si2PO12 (NZSP) to stabilize high-voltage Ni-rich cathodes.
- The modified cathode retains 80% capacity after 511 cycles at 4.7 V and enables a 4 Ah pouch cell to deliver 557 Wh kg–1 with 80.5% retention over 118 cycles.
- This work demonstrates that a Li+/Na+-exchanging interphase can effectively couple interfacial protection with bulk lattice reinforcement for high-voltage Ni-rich cathodes in high-energy lithium batteries.
Readers' thoughts
No reader thoughts yet.
Related papers
- "Spike-Accessed" Polymer-Based Interphase-Engineered Surface-to-Bulk Lattice Stabilization for Ni-Rich Positive Electrodes.Journal of the American Chemical Society · 2026
- Restraining Mechanochemical Failure in High‐Voltage Ni‐Rich Cathode by Coupling Bulk Lattice Pinning With Interphase Self‐ReconstructionAdvanced Energy Materials · 2026
- Lithium–Borate Interphase Enables High‐Rate and Long‐Lifespan Ni‐Rich Layered Oxide CathodesChemSusChem · 2026
- Elastomeric Core-Conductive Shell Slurry Additive Stabilizes High-Voltage NCM811 Cathodes via Mechanical-Electrical Dual Regulation.Advanced science (Weinheim, Baden-Wurttemberg, Germany) · 2026
- Oxyhalide‐Derived Nb‐O‐Cl Interfacial Frameworks for Mitigating Oxygen‐Related Degradation and Facilitating Li + Transport in High‐Voltage Ni‐Rich CathodesAdvanced Energy Materials · 2026
- Covalent-Ionic Bonding Regulation Enables Chemo-Mechanical Stabilization of High-Voltage O3-Type Sodium Layered Oxide Cathodes.Advanced materials (Deerfield Beach, Fla.) · 2026