Materials and Corrosion

The Initiation, Progression, and Stifling of Micro‐Galvanic Corrosion on Cu in Anoxic Aqueous Sulfide Solutions

Jian Chen, Elham Salehi Alaei, Hengyong Nie, Erik Bergendal, Christina Lilja, Mehran Behazin, Peter G. Keech, David W. Shoesmith,

Key points

From the paper's conclusion
  • The growth of Cu 2 S films and the initiation and progression of micro‐galvanic corrosion underneath them were investigated after exposure of Cu to anoxic 0.1 M Cl − solutions containing SH − at concentrations ranging from 10 −5 M to 10 −3 M, for up to 3 years.

Abstract

The growth of Cu 2 S films and the initiation and progression of micro‐galvanic corrosion underneath them were investigated after exposure of Cu to anoxic 0.1 M Cl − solutions containing SH − at concentrations ranging from 10 −5 M to 10 −3 M, for up to 3 years. Post‐exposure surface characterization was performed using scanning electron microscopy (SEM), focused ion beam (FIB) cross‐sectioning, atomic force microscopy (AFM), and surface profilometry. At [SH − ] ≤ 5 × 10 −5 M, a thin and porous Cu 2 S film formed on the Cu surface via general corrosion, favoring surface roughening. Increasing [SH − ] to 5 × 10 −4 or 1 × 10 −3 M resulted in the formation of a compact, crystalline, but non‐uniform Cu 2 S film, under which micro‐galvanic corrosion was observed. A time‐dependent characterization of corrosion damage underlying the Cu 2 S film showed the initiation, propagation, and finally stifling as the film thickened with time. Herein, supported by experimental evidence, a mechanistic pathway for the stifling of the micro‐galvanic corrosion is proposed.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers

The Initiation, Progression, and Stifling of Micro‐Galvanic Corrosion on Cu in Anoxic Aqueous Sulfide Solutions — Science Skim