Microwave–Matter Interactions in Lithium‐Ion Battery Black Mass: Temperature‐Dependent Dielectric Properties and Carbothermal Reduction Pathways
M. Scaglia, A. Zanoletti, M. Gandolfi, F. Bianchi, M. A. Vincenti, Sanad Altarawneh, Jose Rodriguez, Phillip Johnson,
Key points
From the paper's conclusion- These findings show that MW absorption evolves with thermochemical transformations of black mass, highlighting the role of dielectric characterization in optimizing MW‐assisted carbothermal recycling of LIBs.
Abstract
Microwave (MW) heating is a promising alternative to conventional pyrometallurgical processes for recovering strategic metals from spent lithium‐ion batteries (LIBs). However, the temperature‐dependent dielectric behavior of real waste remains poorly understood, limiting the optimization of MW‐assisted recycling processes. In this work, the interaction between MW radiation and black mass from LiCoO 2 (LCO) and LiNi 0 . 6 Co 0 . 2 Mn 0 . 2 O 2 (NMC) cathodes was investigated by combining dielectric characterization, thermal analysis, structural identification, and MW experiments. The complex permittivity was measured from room temperature to 900°C at 910 MHz and 2.45 GHz, using the cavity perturbation method, providing frequency‐resolved datasets linking dielectric evolution with phase transformation in real industrial LIBs black mass. Thermogravimetric (TGA) identified the main thermal events, while X‐ray diffraction (XRD) tracked MW‐induced phase transformations. The results showed that dielectric losses increased markedly in the temperature range 500°C–650°C, corresponding to the onset of carbothermal reduction reactions. In this interval, XRD analysis confirms the transformation of layered cathode phases into Li 2 CO 3 and transition‐metal oxides such as CoO, NiO, and MnO, while TGA reveals the beginning of significant mass loss associated with gas‐evolving reactions. At higher temperatures (> 700°C), further reduction leads to the formation of metallic Co and Ni. The comparison between the two frequencies indicates that 910 MHz promotes deeper and more uniform volumetric heating, whereas 2.45 GHz produces more localized surface heating. These findings show that MW absorption evolves with thermochemical transformations of black mass, highlighting the role of dielectric characterization in optimizing MW‐assisted carbothermal recycling of LIBs.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Selective lithium recovery from spent LiMn2O4 cathodes through carbothermic reduction.Waste management (New York, N.Y.) · 2026
- Selective and sustainable recovery of lithium from black mass via microwave and green leaching techniquesMaterials Science and Engineering B · 2025
- Microwave‐Assisted Leaching and Mixed Oxalates Precipitation as Closed‐Loop NMC532 Recycling ProcessChemElectroChem · 2026
- A Critical Appraisal of Pyrolysis Pretreatment in Lithium‐Ion Battery Recycling: From High‐Temperature Material Transformations to Environmental ImpactChemSusChem · 2026
- Plasma‐Assisted Sustainable Recovery of Critical Minerals from Li‐Ion Battery WasteAdvanced Materials · 2025
- Comparative Reduction Roasting of Mn-Rich Spent NCM Black Mass After NaOH Pretreatment for Selective Metal Recovery: Self-Reduction, CO, and H2 PathwaysMetals · 2026