Mitigating “Electrostrictive” Coupled‐Disruption and Crafting Endogenous Solid‐Liquid Interface Toward Mixed Phosphate Cathode for Sodium‐Ion Batteries
Yian Wang, Mengting Deng, Wenbin Fei, 胡执一, Chengdong Tao, Xiaoping Zhang, Huazhang Guo, Yulei Sui,
Soochow University · Shanghai University
Key points
From the paper's conclusion- This study unveils underlying failure mechanisms for the performance degradation: “electrostrictive” coupled‐disruption driven by charge changes causes the Na + channels closure, while irregular cathode electrolyte interphase (CEI) growth hinders interface Na + diffusion and causes transition metal dissolution.
Abstract
ABSTRACT Na 4 Fe 2 Mn(PO 4 ) 2 (P 2 O 7 ) has received widespread attention due to high energy density and less structural variations. However, its rate capability and cycling performance are far inferior to expectations. This study unveils underlying failure mechanisms for the performance degradation: “electrostrictive” coupled‐disruption driven by charge changes causes the Na + channels closure, while irregular cathode electrolyte interphase (CEI) growth hinders interface Na + diffusion and causes transition metal dissolution. Therefore, halogen elements (F, Cl, Br) are introduced into the material through defect‐engineering. The strong electronegativity of F and the spatial effects of Cl/Br effectively regulate the coordination environment to suppress the coupled‐disruption. Furthermore, the surface halogen elements spontaneously combine with Na + , ultimately forming uniform, surface organic‐rich and interior inorganic‐rich CEI layers. Based on this, the modified material shows high‐rate performance (55.0 mAh g −1 at 200 C) with ultra‐long cycle stability (98% after 20000 cycles at 50 C) and exhibits excellent electrochemical performance in full‐cell and all‐solid‐state battery applications.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Multication Entropy Engineering Enables Fast Sodium Storage in Long-Life Na4Fe3(PO4)2(P2O7)-Based CathodesACS Applied Energy Materials · 2026
- Na4Fe3(PO4)2(P2O7) cathode for sodium-ion batteries: from crystal structure to high-energy-density design and solid-state battery application prospects.Materials horizons · 2026
- Identifying the Relaxative Internal Friction Behavior of Mn2+/Mn3+ Redox in Na4Fe1.5Mn1.5(PO4)2(P2O7) Cathode for Sodium-Ion Batteries.ACS nano · 2025
- A Comprehensive Review of Na4Fe3(PO4)2P2O7 Cathode Materials for Sodium-Ion Batteries: From Crystal Structure and Phase Purification to Modification Strategies Progress.Molecules (Basel, Switzerland) · 2026
- Tailoring Local Sodium Coordination Toward High Initial Coulombic Efficiency Na4Fe3(PO4)2P2O7 Cathodes.Advanced materials (Deerfield Beach, Fla.) · 2026
- Plasma‐Tailored Bulk‐Interface‐Surface Trinity Engineering of Iron‐Based Mixed Phosphate Cathodes for Advanced Sodium Ion BatteriesAdvanced Materials · 2026