Microstructural, Mechanical, and Textural Evolution of Dissimilar Combination of Laser‐Welded Maraging Steel and 4340 Steel
Bharat Behl, Yu Dong, Alokesh Pramanik, Tapas Kumar Bandyopadhyay
Key points
From the paper's conclusion- This study examines and confirms the joint feasibility of their laser welding using mechanical testing, microstructural analysis, and texture analysis, thereby resulting in a sound dissimilar weld joint.
Abstract
Maraging steel, 4340 steel, and their dissimilar combination have similar applications in aerospace, defence, automobile and so on. This study examines and confirms the joint feasibility of their laser welding using mechanical testing, microstructural analysis, and texture analysis, thereby resulting in a sound dissimilar weld joint. The overall yield strength and tensile strength of the weld were increased by 14.4% and 16.67%, respectively, compared to those as‐received maraging steel. However, tensile strength improvement with reference to 4340 steel is 14%. Further, the elongation reached up to 19.7%, leading to a tougher weld joint. Vickers hardness has been determined to be 885 Vickers hardness number (VHN) and 650 VHN in heat‐affected zones (HAZs) on 4340 steel and maraging steel side respectively, which could be attributed to the formation of hard and needle‐like martensite. The presence of austenite was confirmed in the weld zone and HAZ of maraging steel according to X‐Ray diffraction (XRD) and Electron backscattered diffraction (EBSD) analyses, with a clear sign of reverted austenite. This resulted in local softening effect with a decrease in strength. Energy dispersive spectroscopy (EDS) analysis of the tensile fracture surfaces revealed the presence of TiO 2 and Al 2 O 3 inclusions, which were also believed to be the cause of failure by acting as crack initiation points. Texture analysis of martensite phase proved the presence of ℇ‐ fiber, γ‐fiber, and partial presence of α‐fiber in as‐received maraging steel. Additionally, their intensities became lower in the weld zone and HAZ due to phase transformation of both martensite and reverted austenite phases induced by weld thermal cycles.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- The post-heat treatment response of the Laser-Powder Bed Fused 18Ni300 maraging steelJournal of Physics: Conference Series · 2026
- Microstructural Evolution and Mechanical Properties of AA2017 Aluminum Alloy Joints Produced by Rotary Friction Welding and TIG Welding.Materials (Basel, Switzerland) · 2026
- Optimizing impact toughness in Q1100E steel welds via laser-arc hybrid welding energy ratio controlJournal of Materials Research and Technology · 2026
- Investigation of laser-flux cored arc hybrid welding of Q690D high strength steel: weld formation, microstructure evolution and mechanical performanceJournal of Materials Research and Technology · 2025
- Continuous and pulsed TIG welded joint of ASTM A105-AISI 316L steels: Characterization of microstructure, mechanical properties, and fracture analysisJournal of Materials Research and Technology · 2025
- Effect of Welding Speed on the Properties of Laser Beam Welded 3 mm Thick Ti-6Al-4V Butt JointsAdvances in Materials Science · 2026