Effect of TiB 2 Content on Crack Suppression Mechanisms and Microstructural Evolution of IN939 Superalloy Under Pulsed Laser Processing
Yitong Zhang, Changjun Chen, Min Zhang, Haodong Liu, Wei Cao, Dongsheng Wang, Enze Liu, Dunyong Deng
Key points
From the paper's conclusion- The results show that under rapid solidification conditions, TiB 2 particles promote heterogeneous nucleation, reducing the average grain size by approximately 16.82% and significantly weakening the continuity of columnar grains while shortening the interdendritic liquid film channels.
Abstract
High‐γ′ nickel‐based superalloy IN939 is highly susceptible to cracks during laser additive manufacturing, severely limiting its engineering applications. In this work, TiB 2 /IN939 composites were fabricated via pulsed‐wave (PW) laser processing by incorporating TiB 2 particles, and their effects on microstructural evolution, cracking behavior, and friction and wear performance were systematically investigated. The results show that under rapid solidification conditions, TiB 2 particles promote heterogeneous nucleation, reducing the average grain size by approximately 16.82% and significantly weakening the continuity of columnar grains while shortening the interdendritic liquid film channels. The 2 wt.% TiB 2 composite exhibits the lowest local strain level and optimal crack suppression efficiency. The synergistic effect of grain refinement and particle strengthening enhances grain boundary stability and load‐bearing capacity, effectively disrupting crack propagation paths. Furthermore, compared to pure IN939, this composite exhibits an overall superior wear resistance when assessed across both room‐temperature and high‐temperature conditions.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Defect Analysis and Control of In Situ TiB/Ti Laser Cladding Layers on TC4 Titanium AlloyCoatings · 2026
- Synergistic Effects of Carbon/Nitrogen Content and Laser Powder Bed Fusion Parameters on the Hot Cracking Behavior and Microstructural Evolution of a Ni–Co‐Based SuperalloyAdvanced Engineering Materials · 2026
- Weldability Improvement of Additively Manufactured Nickel-Based Superalloy by Controlling W and Si Migration at Solidification Front.Materials (Basel, Switzerland) · 2026
- TiC nanoparticle decoration-induced defect elimination and enhanced mechanical performance of molybdenum via laser powder bed fusionJournal of Alloys and Compounds · 2026
- Mechanistic process–microstructure–cracking correlations in laser powder bed fusion of the Ni-based superalloy IN738Materials & Design · 2026
- Strain-age cracking of a γ′-strengthened nickel-based superalloy additively manufactured by laser powder bed fusionActa Materialia · 2026