Parameterisation of NMC and LFP 4680 cells for electrochemical and thermal modelling
Remus Teodorescu, Nicolai A. Weinreich, Berke Bilgin, Yi Zhuang, Wenzel Prochazka
Key points
From the paper's conclusion- What remains is what a single can node and a single representative particle do not describe: the axial gradient of the NMC can under contact heating, and a gradual decline of the LFP voltage before the knee at 2C, which points to the distribution of particle states in the electrode.
Abstract
An electrochemical-thermal model of the 4680 cylindrical cell is presented: a Doyle-Fuller-Newman model of the electrode stack coupled to a two-node thermal balance of the roll and the can (a thermal DFN, TDFN), solved by an implicit finite-volume scheme. Two cells are parameterised from teardown geometry and open literature, with every value tagged by provenance: the Tesla NMC811/graphite tabless cell and the BYD FC4680 LiFePO4 multi-tab cell. The reaction heat is evaluated at the open-circuit potential of the particle-mean concentration, which restores the heat of mixing. Both sets are calibrated in the same way, with the test fixture identified from the measurement alone. Against the 1C and 2C charge test of Ank et al., the calibrated NMC set follows the mean can temperature within 0.52 and 1.46 K, with a contact heat of 0.94 mOhm matching the authors' estimate for their holder. For the LFP cell, 1C and 2C discharges to 2.0 V were measured on the authors' bench; the fixture conductance (0.337 W/K) follows from the energy balance and the heat capacity (277 J/K) from the cooling. With the end-of-lithiation drop of LiFePO4 restored in the cathode open-circuit potential, the calibrated set follows the can temperature within 0.44 K (1C) and 0.76 K (2C), reproduces the peaks and the relaxation after cut-off. What remains is what a single can node and a single representative particle do not describe: the axial gradient of the NMC can under contact heating, and a gradual decline of the LFP voltage before the knee at 2C, which points to the distribution of particle states in the electrode. The parameter sets (BPX, CSV) and the bench data are openly available.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Impact of Cathode Chemistry and Charging Rates on the Thermal Distribution of Large‐Format Lithium‐Ion Batteries: A Fully Coupled 3D Electrochemical–Thermal Modeling ApproachEnergy Technology · 2026
- Experimental and numerical electro-thermal analysis of a pouch cell battery accounting for connection bar effects via equivalent boundary conditions on tabsJournal of Energy Storage · 2026
- Design and Performance of the BYD LFP/Graphite 4680 Cylindrical CellJournal of The Electrochemical Society · 2025
- Modeling the variability of thermal runaway behavior in large-format cylindrical cells with NMC-811 and LFP cathodes: A simulation studyJournal of Power Sources · 2026
- A Physics-Informed TCN-LSTM Approach for Interpretable Internal Temperature Estimation of NMC811 Lithium-Ion BatteriesBatteries · 2026
- Bridging the Safety-Performance Gap: A Comparative Study of Graphite Versus Niobium Tungsten Oxide Anodes and Carbonate Versus Ether Electrolytes for Lithium-Ion BatteriesACS Applied Energy Materials · 2026