arXivPreprintOpen accesscond-mat.dis-nn

Quantifying the Kinetic and Thermodynamic Origins of the Glass-Forming Ability in Metals

Weiwei Jin, Jinpeng Fan, Mark D. Shattuck, Corey S. O'Hern

Key points

From the paper's conclusion
  • We show that the thermodynamic contribution to $\mathcal{K}_{\rm X}$ dominates the kinetic contribution over the range of cooling rates that we consider.

Abstract

The glass-forming ability (GFA) of a metallic liquid can be quantified by the critical cooling rate $R_c$, below which it crystallizes upon cooling. $R_c$ is determined by the competition between $R$ and the crystallization rate $\mathcal{K}_{\rm X}$. Here, we calculate $R_c$ and $\mathcal{K}_{\rm X}$ in model pure metals and alloys with BCC/B2 and FCC equilibrium crystal structures. Using classical nucleation theory and independently calculated crystal growth rates, we evaluate $\mathcal{K}_{\rm X}=(IU^3)^{1/4}$ at $T=0.8T_m$, where $I$ and $U$ are the nucleation and growth rates and $T_m$ is the melting temperature. We find a strong positive correlation between $\mathcal{K}_{\rm X}$ and $R_c$ over eleven orders of magnitude. We decompose $\mathcal{K}_{\rm X}$ into a product of a kinetic contribution, involving atomic cluster attachment and diffusion, and a thermodynamic contribution. We show that the thermodynamic contribution to $\mathcal{K}_{\rm X}$ dominates the kinetic contribution over the range of cooling rates that we consider. The nucleation barrier $\Delta G_c \sim \tilde\gamma^3/\Delta\tilde\mu^2$, where $\tilde\gamma$ is the reduced effective liquid--crystal interfacial free energy and $\Delta\tilde\mu$ is the reduced bulk driving force, determines the magnitude of the thermodynamic contribution. The relative importance of $\tilde\gamma$ and $\Delta\tilde\mu$ depends on the material: a large interfacial free energy can suppress nucleation in some systems, whereas a weak bulk driving force can inhibit crystallization in others. Analyses of the structural and chemical order show that better glass formers have enhanced structural frustration, more icosahedral-like and less crystal-like local environments, and a larger chemical-order mismatch between the supercooled liquid and crystal phases.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers

Quantifying the Kinetic and Thermodynamic Origins of the Glass-Forming Ability in Metals — Science Skim