Comparative Evaluation of the Shear Bond Strength of Different Core-Veneer Restorative Systems: An In Vitro Study.
Kamaldeep Sharma, Reeta Jain, Gurmeet K Virdi, Sumit Chopra, Shanta Chopra, Manmohit Kumar
Department of Prosthodontics, Genesis Institute of Dental Sciences and Research, Punjab, IND. · Department of Orthodontics, Genesis Institute of Dental Sciences and Research, Punjab, IND.
Key points
From the paper's conclusion- Within the limitations of this in vitro study, the conventional Ni-Cr/IPS classic system had higher baseline nominal shear bond strength compared to the other core-veneer systems under immediate loading conditions. Because each restorative group utilised material-specific interfacial bonding protocols and distinct veneering ceramics, these findings reflect integrated system-level performance rather than isolated intrinsic core properties. Furthermore, the reported bond values represent nominal, unaged baseline values obtained without failure-mode classification. Long-term studies incorporating artificial ageing, cyclic fatigue loading, and fractographic analysis are essential before clinical recommendations can be drawn.
Abstract
INTRODUCTION: Porcelain-fused-to-metal (PFM) systems have long been the gold standard for fixing partial dentures (FPDs). The bond between the ceramic and the core depends on various factors, such as the oxide layer, the thermal expansion coefficients, and the alloy's microstructure. The longevity of any bilayer restoration depends critically on the bond strength between the aesthetic porcelain and the underlying core material. Given that the interfacial bond strength dictates the clinical survival of bilayer restorations, this study evaluated and compared the nominal shear bond strength across four distinct core-veneer restorative systems. METHODOLOGY: A total of 40 standardised rectangular specimens (25 mm × 3 mm × 0.5 mm) of different alloy combinations were fabricated and equally divided into four groups. Group 1 is conventional cast Ni-Cr alloy, Group 2 is conventional cast Co-Cr alloy, Group 3 is direct metal laser sintered (DMLS) Co-Cr alloy, and Group 4 is CAD/CAM milled zirconia. Conventional Ni-Cr (Group 1) and Co-Cr (Group 2) core alloy specimens were fabricated using rectangular wax patterns obtained from smooth casting wax sheets of 0.5 mm thickness. Porcelain buildup was applied to all specimens in the central 8 mm, leaving 8.5 mm on either side, to a uniform thickness of 1 mm, followed by a ceramic firing cycle as recommended by the manufacturer. Each prepared specimen of veneered porcelain with core structure was subjected to shear force at a crosshead speed of 1mm/min on a universal testing machine (UTM). Loading was done till fracture occurred. The shear bond strength was calculated in megapascals (MPa). RESULTS: Maximum shear bond strength of 25.67 MPa was observed in Group 1, while a minimum of 2.54 MPa was observed in Group 2. To compare all groups, a one-way ANOVA was performed, which revealed a highly significant difference (p < 0.001) among the study groups. To make individual pairwise comparisons, Tukey's HSD post-hoc test was applied. This test revealed a highly significant difference in the mean shear bond strength between Group 1 and all other study groups. However, the comparison among all remaining study groups was not statistically significant. CONCLUSION: Within the limitations of this in vitro study, the conventional Ni-Cr/IPS classic system had higher baseline nominal shear bond strength compared to the other core-veneer systems under immediate loading conditions. Because each restorative group utilised material-specific interfacial bonding protocols and distinct veneering ceramics, these findings reflect integrated system-level performance rather than isolated intrinsic core properties. Furthermore, the reported bond values represent nominal, unaged baseline values obtained without failure-mode classification. Long-term studies incorporating artificial ageing, cyclic fatigue loading, and fractographic analysis are essential before clinical recommendations can be drawn.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- In vitro comparison of enamel shear bond strength to four restorative substrates used in resin-bonded prostheses.Medicine · 2026
- Evaluation of the bond strength of composite resins with distinct properties to short fiber-reinforced composite resins of different viscosities.Odontology · 2026
- Effect of Prosthesis and Pickup Materials on the Bond Strength of Temporary Cylinders in Full-Arch Implant-Supported Interim Prostheses.The International journal of oral & maxillofacial implants · 2026
- Fracture resistance of endodontically treated maxillary premolars restored with different bi-layered core and occlusal overlay materials: an in vitro study.BMC oral health · 2026
- Redefining the role of custom post and core systems: Moving beyond retention to structural reinforcement of severely compromised teeth: An in vitro study.Journal of prosthodontics : official journal of the American College of Prosthodontists · 2026
- Interfacial Bond Strength of CAD/CAM Resin Composites on Dentin vs. Composite Substrates: Influence of Dual-Cure and Self-Adhesive Resin CementsPolymers · 2026