Effects of Component Prechilling and Ambient Temperature on the Handling and Thermal Characteristics of Two Polymethylmethacrylate (PMMA) Bone Cements.
Szoradi Gergo, Andrei-Marian Feier, Octav M Russu, Sandor G Zuh, Tudor S Pop
Department M4 Clinical Sciences, Orthopedics and Traumatology I, George Emil Palade University of Medicine, Pharmacy, Science, and Technology of Targu Mures, Mures, ROU. · Department M4 Clinical Sciences, Orthopedics and Traumatology I, George Emil Palade University of Medicine, Pharmacy, Science, and Technology of Targu Mures, Targu Mures, ROU.
Key points
From the paper's conclusion- Lower component and ambient temperatures prolonged the handling and hardening intervals and reduced peak core temperatures in this bench model. Component temperature produced larger descriptive changes than the 5 °C difference in ambient temperature. The completed factorial ANOVA confirmed significant main effects for component temperature, ambient temperature, and formulation without significant interaction effects. Lower component and ambient temperatures prolonged handling and hardening intervals and reduced peak core temperatures in this exploratory bench model. However, given the small sample size, non-randomized testing sequence, subjective handling endpoint, and simplified cylinder geometry, these findings do not establish a clinical cooling protocol. Clinical recommendations require further confirmation using verified commercial products, clinically representative cement geometries, and direct interface-temperature measurements.
Abstract
BACKGROUND AND OBJECTIVES: Polymethylmethacrylate (PMMA) bone cement remains a very important part of implant fixation in joint arthroplasty. Surgeons must find a way to balance the working time with the risk of excessive heat generated through polymerization that may contribute to thermal necrosis at the cement-bone interface. Handling and heat generation depend on the temperature of the cement components and the surrounding environment. This bench study examined component prechilling and ambient temperature in two arthroplasty cement formulations. METHODS: Sixteen batches of Simplex P (Stryker Corporation, Kalamazoo, MI, USA) and 16 batches of an antibiotic-loaded Simplex formulation were evaluated in a 2 × 2 temperature design: components conditioned at 21 °C or 4 °C and specimens cured at ambient temperatures of 21 °C or 16 °C. Cement was mixed manually for 30 s and formed into two 2-cm cylinders per batch. The recorded endpoints were an operational working-time measure, indentation-defined hardening time, and peak core temperature. RESULTS: With Simplex P, prechilling at an ambient temperature of 21 °C increased mean working time from 210.4 to 315.6 s and hardening time from 645.2 to 912.8 s, while peak temperature decreased from 78.4 to 62.1 °C. The combined 4 °C component and 16 °C ambient condition produced a working time of 398.1 s, a hardening time of 1054.3 s, and a peak temperature of 60.4 °C. Corresponding values for antibiotic-loaded Simplex were 228.1 s, 682.4 s, and 76.2 °C under baseline conditions and 418.5 s, 1098.6 s, and 59.1 °C under the combined-cold condition. CONCLUSIONS: Lower component and ambient temperatures prolonged the handling and hardening intervals and reduced peak core temperatures in this bench model. Component temperature produced larger descriptive changes than the 5 °C difference in ambient temperature. The completed factorial ANOVA confirmed significant main effects for component temperature, ambient temperature, and formulation without significant interaction effects. Lower component and ambient temperatures prolonged handling and hardening intervals and reduced peak core temperatures in this exploratory bench model. However, given the small sample size, non-randomized testing sequence, subjective handling endpoint, and simplified cylinder geometry, these findings do not establish a clinical cooling protocol. Clinical recommendations require further confirmation using verified commercial products, clinically representative cement geometries, and direct interface-temperature measurements.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Converging Materials, Chemistry, and Interface Design Toward Mitigating Exothermic Heat for Clinically Safer PMMA Bone CementsAdvanced Functional Materials · 2026
- Redefining injectable PMMA bone cement: Beta-tricalcium phosphate integration for bioactive and osteoconductive performance for minimally invasive applications.Bio-medical materials and engineering · 2026
- Function-integrated injectable poly(methyl methacrylate) bone cement engineered with silver-templated mesoporous calcium-silicate nanoparticles via a chitosan-glycerophosphate hydrogel.RSC advances · 2026
- Advances in TCP-Modified PMMA Bone Cements: Relating Microstructure to Mechanical, Biological and Functional Performance-Systematic Review.Materials (Basel, Switzerland) · 2026
- Dual-Setting Magnesium Phosphate Bone Cement with Improved Handling Through the Integration of Chitosan-Derived Hydrogels.Journal of functional biomaterials · 2026
- PMMA-co-calcium methacrylic phyllosilicate hybrid bone cements induce biomimetic mineralization.Colloids and surfaces. B, Biointerfaces · 2026