Adhesion of Bioactive Glass Nanoparticle-Modified Biodentine Under Simulated Early and Aged Conditions.
Hernán Coaguila-Llerena, Camila Corral-Núñez, Cristian Covarrubias, Karen Abt-Calle, Camila Lizárraga-Gutiérrez, Gabriela Castro-Núñez, José Giancarlo Tozo-Burgos, Wilfredo Escalante-Otárola
School of Dentistry, Catholic University of Santa Maria - UCSM, Arequipa, Peru. · Department of Restorative Dentistry, School of Dentistry, Universidad de Chile - UCHILE, Santiago, Chile.
Key points
From the paper's conclusion- Incorporation of nBG into BD improved apparent shear bond strength of the bonded cement-adhesive-composite assembly to Scotchbond Universal Plus when applied using the self-etch strategy under both early and aged conditions and altered the crystalline surface morphology.
Abstract
OBJECTIVE: This study evaluated the adhesion of Biodentine (BD) modified with 2% bioactive glass nanoparticles (nBG/BD) under simulated early and aged conditions. METHODS: Acrylic blocks (n = 10 per group) were filled with nBG/BD or BD. Groups were assigned according to adhesive strategy: Scotchbond Universal Plus applied using etch-and-rinse (ER-nBG/BD; ER-BD) or self-etch (SE-nBG/BD;SE-BD) approaches. Adper Single Bond 2 served as a control using the etch-and-rinse strategy (ASB-nBG/BD; ASB-BD). Bond strength (MPa) was measured using a universal testing machine, and fracture depth (mm) was assessed using cone-beam computed tomography under early (24 hours) and aged conditions. Surface morphology and elemental composition were evaluated using scanning electron microscopy and energy dispersive spectroscopy. Data were analysed using 1-way or Welch ANOVA followed by Tukey or Dunnett T3 post hoc tests (α = 0.05). RESULTS: Under early conditions, SE-nBG/BD showed the highest bond strength (P < .05). SE-BD, SE-nBG/BD and ASB-BD exhibited the greatest fracture depths, with no differences among them (P > .05). Under aged conditions, bond strength increased in all groups (P < .05), SE-nBG/BD and SE-BD showed the highest bond strength (P < .05), whereas SE-BD exhibited the greatest fracture depth (P < .05). Scanning electron microscopy analysis revealed that nBG/BD exhibited more cubic-, needle- and rod-shaped crystals than BD. Energy dispersive spectroscopy analysis indicated greater chlorine detection in nBG/BD. CONCLUSION: Incorporation of nBG into BD improved apparent shear bond strength of the bonded cement-adhesive-composite assembly to Scotchbond Universal Plus when applied using the self-etch strategy under both early and aged conditions and altered the crystalline surface morphology.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Diode laser-activated sodium fluoride and galla chinensis extract as dentin biomodifiers: Effect on microhardness, resin tag length, and shear bond strength of universal adhesive to caries-affected dentin.Pakistan journal of medical sciences · 2026
- Effect of chitosan and bioactive glass nanoparticles on the push-out bond strength of epoxy resin-based sealer: an in-vitro study.BMC oral health · 2026
- Comparison of Dentin Bond Strength Between a Bioactive Resin-Modified Glass Ionomer Cement and a Conventional Self-Adhesive Resin Cement: An In Vitro Study.Cureus · 2026
- Comparative Evaluation of the Push-Out Bond Strength and Antimicrobial Efficacy of Biodentine and Bioactive Bone Cement as Root-End Filling Materials: An In Vitro Study.Cureus · 2026
- Influence of Adhesive Strategies on the Bond Strength and Fracture Behaviour of Biodentine™ XP to Flowable Bulk-Fill CompositeJournal of Composites Science · 2026
- Sepiolite and Zirconia Nanoparticles Doped with Erythrosine: Adhesive Bond Strength and Antimicrobial Performance in Primary Carious Dentin.Pakistan journal of medical sciences · 2026