Effect of staining solutions on the surface properties and color stability of conventional and CAD/CAM interim restorative materials.
Otavio Marino Dos Santos-Neto, Marisa Alves Lúcio Ferreira, João Paulo do Vale-Souza, Ricardo Alexandre Zavanelli, José Vitor Quinelli Mazaro, Adriana Cristina Zavanelli
Federal University of Santa Catarina, Florianópolis, SC, Brazil. · São Paulo State University (UNESP), School of Dentistry, Araçatuba, SP, Brazil.
Key points
From the paper's conclusion- Milled CAD/CAM interim resins demonstrated superior surface and color stability compared with conventional and 3D-printed materials. Red wine negatively impacted the surface integrity of 3D-printed resins, while bis-acryl materials were most susceptible to clinically unacceptable staining.
Abstract
BACKGROUND: The long-term esthetic and physical performance of interim restorations depends on the material's resistance to the oral environment; however, the impact of common beverages on newer CAD/CAM and 3D-printed resins remains unclear. The purpose of this in vitro study was to evaluate the surface roughness (ΔRa), microhardness (KHN), and color stability (ΔE00) of 5 interim restorative materials after immersion in different staining solutions. MATERIALS AND METHODS: Specimens (N=200, n=10 per group) were fabricated from autopolymerizing acrylic, heat-polymerized acrylic, bis-acryl, milled CAD/CAM (PMMA), and 3D-printed resins. After 30 days of distilled water storage, baseline measurements were recorded. Specimens were then immersed in coffee, a cola-based beverage, red wine, or artificial saliva for 14 days, with daily solution renewal. Data were analyzed using ANOVA, Kruskal-Wallis, paired t-tests, and Wilcoxon tests as appropriate (α=.05). RESULTS: Red wine resulted in significant differences in surface roughness (P=.018), increasing ΔRa for the 3D-printed resin (0.93 ± 1.25) while decreasing it for milled PMMA (-1.01 ± 1.20). Microhardness significantly decreased for most material-solution combinations after 14 days (P<.05). Coffee and red wine caused the greatest color changes, with the bis-acryl resin exhibiting ΔE00 values up to 4.05 ± 2.09, exceeding the clinical acceptability threshold (1.8). CAD/CAM-based materials generally demonstrated greater color stability than conventional materials. CONCLUSIONS: Milled CAD/CAM interim resins demonstrated superior surface and color stability compared with conventional and 3D-printed materials. Red wine negatively impacted the surface integrity of 3D-printed resins, while bis-acryl materials were most susceptible to clinically unacceptable staining.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Evaluation of Color Stability and Surface Properties of Different CAD/CAM Materials: An In vitro Study.Nigerian journal of clinical practice · 2026
- Surface Roughness and Color Stability of 3D-Printed Dental Resin Materials Under the Influence of Different Beverages.Journal of functional biomaterials · 2026
- Effect of ultrasonic chemical cleaning solutions on different dental interim restoration material properties. Part I: Physical properties of color stability and surface roughness.The Journal of prosthetic dentistry · 2026
- Color Stability and Surface Roughness of CAD/CAM Hybrid Ceramics and Resin Composites After Simulated Toothbrushing in Coffee: An In Vitro StudyApplied Sciences · 2026
- Color stability of CAD/CAM and additively manufactured resin materials: influence of surface treatment and layer thickness - an in vitro studyThe Saudi Dental Journal · 2026
- Color Stability and Flexural Strength of Temporary Prosthetic Materials under the Influence of Staining Substances.The journal of contemporary dental practice · 2025