Optimizing the synthesis of bioactive glass for endodontic applications.
Tahir Yusuf Noorani, Eyas Abuhijleh, Matheel Al-Rawas, Sohaib Fadhil Mohammed, Manahil Maqbool, Mohmed Isaqali Karobari
Department of Conservative Dentistry and Endodontics, Saveetha Dental College and Hospitals, Saveetha Institute of Medical and Technical Sciences, Saveetha University, Chennai, Tamil Nadu, India. · Department of Clinical Sciences, Center of Medical and Bio-Allied Health Sciences Research, College of Dentistry, Ajman University, Ajman, United Arab Emirates.
Key points
From the paper's conclusion- The addition of ammonia solution improved the morphology and structural homogeneity of sol-gel-derived BG 58S without affecting its chemical composition. This study lays the basis for the synthesis of BG 58S for incorporation into novel endodontic sealers, pulp capping agents, and retrograde filling materials.
Abstract
OBJECTIVE: The objective of the study was to optimize the sol-gel synthesis of bioactive glass (BG) 58S by evaluating the influence of an ammonia catalyst on its textural, morphological, and structural properties. MATERIALS AND METHODS: BG 58S was synthesized using a modified sol-gel technique. Two groups were prepared: Group I (0 mL ammonia) and Group II (1.5 mL ammonia). Following aging and calcination at 600°C, both powders were characterized using scanning electron microscopy-energy-dispersive X-ray spectroscopy (SEM-EDX), Fourier Transform Infrared Spectroscopy (FTIR), X-ray Diffraction (XRD), and Brunauer-Emmett-Teller (BET) analyses. RESULTS: SEM images of Group I revealed highly irregular, angular, and plate-like microparticles with smooth surfaces. In contrast, Group II demonstrated loosely packed, fine, spherical nanoparticles aggregated into clusters. EDX and FTIR confirmed the presence of a silicate network in both groups. XRD confirmed that amorphous glass phase was present in both groups, with Group II having a broader halo. BET analysis showed that both materials were type IV mesoporous structures, and a more homogeneous pore network with fewer large mesopores was present in Group II. CONCLUSION: The addition of ammonia solution improved the morphology and structural homogeneity of sol-gel-derived BG 58S without affecting its chemical composition. This study lays the basis for the synthesis of BG 58S for incorporation into novel endodontic sealers, pulp capping agents, and retrograde filling materials.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Controlled sol-gel nanoassembly of Au25(SR)18 nanoclusters for structural and functional integration.Frontiers in chemistry · 2026
- The Significant Impact of the Evolution of Porous Architecture in Sol-Gel Processed-Nanoscale ZnO-Bearing Bioactive Glass in a Physiological Environment.International journal of nanomedicine · 2026
- Cranberry-coated mesoporous bioactive glass for bone tissue regeneration: Biofilm and osteogenic analysis in vitro.Archives of oral biology · 2026
- Sol-Gel Process Optimization of Transparent Silica Aerogels: Regulating Nanostructure to Enhance Optical Transmittance.Nanomaterials (Basel, Switzerland) · 2026
- Surfactant-free synthesis of copper-incorporated bioactive glass nanoparticles for controlled ion release, antibacterial activity, and apatite-forming ability.Dental materials : official publication of the Academy of Dental Materials · 2026
- Sustainable Production of Supramolecular Hydrogels Based on Bioactive Glass/Monoammonium Salt of Glycyrrhizic Acid/Chitosan Assemblies for Biomedical ApplicationsCeramics · 2026