Influence of surface-conditioning strategies on the shear bond strength of veneering ceramic to aged and non-aged zirconia frameworks fabricated with milling and 3D-printing.
Selin Çakır, Özay Önöral
Department of Prosthodontics, Faculty of Dentistry, Near East University, Nicosia, Cyprus.
Key points
From the paper's conclusion- Surface-conditioning strategy had the greatest influence on zirconia-veneer bond performance, with TSC producing the highest SBS values regardless of fabrication technique. Although LCM exhibited statistically higher SBS values than CNC, this difference was modest and both techniques demonstrated comparable bond performance from a practical perspective. LCM specimens also exhibited higher surface roughness than CNC specimens.
Abstract
PURPOSE: The purpose of this in vitro study was to investigate how various surface-conditioning strategies and thermal aging affect the shear bond strength (SBS) of aged and non-aged zirconia frameworks fabricated through different techniques. MATERIALS AND METHODS: A total of 208 rectangular frameworks were fabricated by computer numerical control (CNC) and lithography-based ceramic manufacturing (LCM) techniques. The specimens were randomly allocated into 4 groups according to the surface-conditioning strategy applied on the veneering surface: no surface conditioning (C), airborne-particle abrasion (APA), tribochemical silica-coating (TSC), and grinding (GRD). Surface topographies were scrutinized under a scanning electron microscope, surface roughness (Ra) was measured, and the SBS test was performed. Failure patterns were evaluated. Data were statistically analyzed (α = 0.05). RESULTS: Three-way ANOVA showed significant main effects of fabrication technique, surface-conditioning, and thermal aging (P < .001 for all) on SBS, with no significant three-way interaction (P = .225). LCM showed higher SBS than CNC (24.02 vs 22.04 MPa), TSC yielded the highest value (32.28 MPa), and aging reduced overall SBS from 27.20 to 18.85 MPa. Two-way ANOVA showed significant main effects of fabrication technique and surface-conditioning on Ra, with significant interaction between them (P < .001 for all). CONCLUSION: Surface-conditioning strategy had the greatest influence on zirconia-veneer bond performance, with TSC producing the highest SBS values regardless of fabrication technique. Although LCM exhibited statistically higher SBS values than CNC, this difference was modest and both techniques demonstrated comparable bond performance from a practical perspective. LCM specimens also exhibited higher surface roughness than CNC specimens.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Influence of Zirconia Type and Surface Treatment on the Shear Bond Strength Between Veneering Porcelain and Zirconia.Dentistry journal · 2026
- The effect of using 40% HF treatment on the shear bond strength of the zirconia surface in comparison to conventional surface treatment methods.Journal of lasers in medical sciences · 2026
- Evaluation of the effect of sandblasting and laser surface treatments on the shear bond strength of zirconia with different yttria content using resin cement.Odontology · 2026
- Shear bond strength of 3D-printed zirconia with customized surface texture when compared with milled zirconia and glass-ceramicDigital Dentistry Journal · 2026
- Evaluation of Bond Strength of Different Surface-Treated Translucent Zirconia Blocks Luted with Universal Resin Cement to Glass-Reinforced Core Composite Before and After Aging: An In vitro Study.Journal of pharmacy & bioallied sciences · 2026
- Influence of surface treatment and simulated aging on the shear bond strength of different luting agents to zirconia.Dental and medical problems · 2026