H+ and Li+ Ion Intercalation of Electrodeposited Tungsten Oxide Thin Films
Gamze Atak
Hacettepe University
Key points
From the paper's conclusion- Tungsten oxide (WO3) thin films were deposited by electrodeposition using Na2WO4.2H2O with deionized water, H2O2 and HClO4 electrolyte solution at -0.7 V versus Ag/AgCl with a continuous potential.
Abstract
Tungsten oxide (WO3) thin films were deposited by electrodeposition using Na2WO4.2H2O with deionized water, H2O2 and HClO4 electrolyte solution at -0.7 V versus Ag/AgCl with a continuous potential. Their electrochromic properties were analyzed in 0.5M H2SO4 and 0.5M LiClO4/PC electrolytes to understand the H+ and Li+ ion intercalation/de-intercalation mechanism. The bleached and colored transmission measurements were carried out after 50th CV and coloration efficiency of the films were calculated as ΔT= 60 % and CE =28.5 cm2/C for 0.5 M H2SO4 and ΔT= 50.3 % and CE =76.5 cm2/C for 0.5 M LiClO4/PC, respectively. The diffusion coefficient was calculated to be 1.59 × 10⁻⁹ cm²·s⁻¹ in 0.5 M H₂SO₄ and 6.19 × 10⁻¹⁰ cm²·s⁻¹ in 0.5 M LiClO₄/PC. Furthermore, memory effect experiments were carried out to investigate the influence of electrolyte type. The comparative results indicate that Li⁺-based electrolytes are more advantageous for low-energy electrochromic applications requiring a pronounced memory effect, whereas proton-based electrolytes are more suitable for applications demanding fast and high optical contrast. Additionally, optical (UV-Vis-NIR spectrophotometer), morphological (SEM & EDX), and Mott-Schottky measurements were performed for the characterization of the WO3 films.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Electrolyte-Regulated Ion Accommodation and Microstructural Stability in WO3 Electrochromic Thin Films.Micromachines · 2026
- Research Progress on Electrochromic Properties of WO3 Thin FilmsCoatings · 2025
- Interface Engineering of Hydrated Tungsten Oxide via Carbon Nitride for Durable Electrochromic Energy Storage.ACS applied materials & interfaces · 2026
- Investigation of the Effect of O2/Ar Ratio on Flexible WO3 Electrochromic Films Prepared by Magnetron Sputtering and Performance Optimization via Ti Doping.ACS omega · 2026
- Engineering the Structure-Performance Relationship of WO3 Thin Films Through PVP-Mn Synergy for Electrochromic Applications.Polymers · 2026
- Atomic Layer Deposition-Enabled Ultrathin Al2O3 Interfacial Layers for Ion-Regulated Durable Flexible WO3 Electrochromic FilmsCoatings · 2026