Stabilization of Acidic Uranium Tailings Residue Using a Cement-Fly Ash-Zero-Valent Iron Composite: Mechanical Performance and Long-Term Leaching Behavior.
Jie Niu, Yang Wang, Tongxin Duo, Dong Zhang, Mumtaz Khan, Xiaochao Liu, Dong Ji
Beijing Research Institute of Chemical Engineering and Metallurgy, China National Nuclear Corporation, Beijing 101149, China. · Zhonghe Mining Technology Co., Ltd., Beijing 100022, China.
Key points
From the paper's conclusion- This study developed a multifunctional stabilization/solidification strategy combining Portland cement, fly ash (FA), and zero-valent iron (Fe0) for acidic uranium tailings residue generated after sulfuric-acid extraction.
Abstract
Acid-leached uranium tailings residues present a long-term management challenge because uranium mobility, sulfur-driven acidification, and poor structural stability must be controlled simultaneously. This study developed a multifunctional stabilization/solidification strategy combining Portland cement, fly ash (FA), and zero-valent iron (Fe0) for acidic uranium tailings residue generated after sulfuric-acid extraction. The residue contained approximately 0.011% U and high Si-Al and sulfur contents, and showed a marginal acid-base balance, with an acid-neutralization capacity of 83.3 and maximum potential acidity of 75.3. Fine particles exhibited higher porosity and greater uranium release. Cement-to-residue ratio, water-to-cement ratio, curing age, FA replacement, and Fe0 addition were systematically evaluated. A cement-to-residue ratio of 3:7 and water-to-cement ratio of 0.6 yielded a 28 d unconfined compressive strength of 28.7 MPa. Incorporation of 15-25% FA with 1% Fe0 maintained strength at approximately 30 MPa, while five freeze-thaw cycles caused only a 2.79% strength loss. Direct Fe0 treatment reduced cumulative uranium release by approximately 78%. Cement solidification maintained uranium concentrations below 10 μg L-1 during 90 d leaching under acidic, neutral, and alkaline conditions, corresponding to >99% suppression relative to untreated residue, while cement + Fe0 further reduced uranium release to <1 μg L-1. Sulfate release was reduced to less than one-third of that from untreated residue. Overall, cement, FA, and Fe0 provided complementary structural, matrix-modifying, and uranium-reactive functions, enabling simultaneous control of mechanical integrity and contaminant mobility.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Preparation of composite ceramics with microwave–sintered uranium tailings for fixing Sr/Nd binary radionuclidesMaterials & Design · 2026
- Effect of crushed concrete waste on leaching behaviour of alum shale: A layered column study.Waste management (New York, N.Y.) · 2026
- Mechanical Properties and Leaching Characteristics of BF-MICP Solidified/Stabilized Ion-Type Rare Earth Tailings.Microorganisms · 2026
- Elucidating cesium solidification and stabilization mechanisms in nano-gamma-alumina modified cementitious matrices under realistic conditionsnpj Materials Degradation · 2026
- Bioash-Based Stabilization/Solidification for Heavy Metal(oid) Soil Remediation: A Case Study in Northern SwedenMaterials · 2026
- Strength and leaching characteristics of stabilized ionic rare earth tailings by microbially induced calcium carbonate precipitationPLoS ONE · 2026