Potassium Sorbate-Modified Adhesive Layers in Greaseproof Cardboard Inserts: Mechanical Performance, Migration Behaviour and Technological Validation
Marcin Cichosz, Joanna Wyrwas, Mieczysława Katarzyna Nath, Urszula Kiełkowska
Key points
From the paper's conclusion- Overall migration to modified polyphenylene oxide (MPPO; Tenax®) was determined at an additive concentration of 4.0% (w/w), using ten measurements per modifier.
Abstract
Paper- and cardboard-based food-contact materials require solutions that combine mechanical integrity, controlled migration and technological simplicity. This study evaluated greaseproof cardboard inserts in which the aqueous adhesive layer was modified with sodium alginate, chitosan or potassium sorbate. Initial formulation screening comprised eight concentrations (0.5–4.0% (w/w)) for each modifier, with ten adhesive-joint strength measurements per formulation (240 measurements in total). Overall migration to modified polyphenylene oxide (MPPO; Tenax®) was determined at an additive concentration of 4.0% (w/w), using ten measurements per modifier. Further experiments evaluated adhesive application side, adhesive dosage (9 and 15 g·m−2), creasing intensity (0–20 crease lines), and potassium sorbate concentrations of 4.30, 4.55 and 4.90% (w/w). Among the tested modifiers, potassium sorbate combined relatively high mechanical performance with lower overall migration: normalised breaking force remained within 144.2–181.6 N·m−1 across the initial screening range, and overall migration at 4.0% (w/w) was the lowest among the three modifiers (3.61 ± 0.38 mg·dm−2). Additional migration validation yielded 4.678 ± 0.292 and 4.779 ± 0.158 mg·dm−2 for the 4.30 and 4.55% formulations, respectively, whereas the 4.90% formulation showed substantially higher migration (8.737 ± 0.204 mg·dm−2) and reduced breaking force below the internal technological acceptance criterion. Increasing adhesive dosage from 9 to 15 g·m−2 significantly increased migration within both investigated exposure protocols. The 4.30–4.55% (w/w) potassium sorbate range was identified as a preliminary technological window under the investigated conditions. Given the limited number of independent production batches and the absence of formal statistical optimisation, this interval should not be interpreted as a statistically established optimum or a generalisable formulation limit. Antimicrobial efficacy and shelf-life extension were not investigated.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Potassium Sorbate-Functionalized Food-Contact Inserts: Effects on Total Microbial Load and Sensory Acceptability of Model Food Products.Materials (Basel, Switzerland) · 2026
- Activating Kraft Paper by Coating With Guar Gum Incorporated With Curcumin for Butter Packaging ApplicationJournal of Food Process Engineering · 2026
- Tackling the “Stickies” Problem When Recycling Pressure-Sensitive Adhesives with Degradable, Hydrophilic Thioester Copolymer NetworksACS Applied Polymer Materials · 2026
- Citric Acid-Urea Modification of Dual-Plasticized Starch Adhesives for Medium-Density Fiberboard Manufacturing.Polymers · 2026
- Chitosan-Based Adhesive for Fabrication of Organic–Inorganic Hybrid Wood Composites with Robust Interfacial Bonding and Flame RetardancyACS Sustainable Chemistry & Engineering · 2025
- Tobacco Stem Powder‐Modified Phenolated Kraft Lignin‐Based Phenol–Formaldehyde Adhesive for Wood BondingJournal of Applied Polymer Science · 2026