Waste Stone Wool as a Co-Precursor in Natural Pozzolan-Based Alkali-Activated Materials: Balancing Performance, Resource Efficiency, and Carbon Intensity
Kübra Ekiz Barış
Key points
From the paper's conclusion- Within the defined material-input boundary, SW replacement reduced NP consumption and the material-based carbon indicator, with the lowest carbon intensity per unit compressive strength (0.0113 kg CO2-eq./MPa) obtained for SW30-7.5M.
Abstract
Within the literature reviewed, no systematic study was identified that evaluates waste stone wool (SW) as a partial replacement for natural pozzolan (NP) while varying both SW content and NaOH concentration in the same alkali-activated material (AAM) mixture. To address this gap, this study examined SW replacement levels of 0–40 wt.% and NaOH concentrations of 5, 7.5, and 10 M. Fresh-state behavior, physical and mechanical properties, drying shrinkage, pore structure, and material-based environmental indicators were evaluated. Increasing SW replacement level reduced flowability, while mixtures containing up to 30% SW showed improved hardened-state performance. SW30-7.5M exhibited the best overall performance, with compressive and flexural strengths of 16.13 and 3.41 MPa, respectively, total porosity of 15.07%, and ultrasound pulse velocity of 3.19 km/s. It also showed the lowest 63-day drying shrinkage magnitude, with a reported value of −1014.9 × 10−6 mm/mm. Mercury intrusion porosimetry (MIP) analysis of this mixture gave an MIP porosity of 14.03% and an average pore diameter of 0.24 µm. X-ray diffraction (XRD) and Fourier transform infrared spectroscopy (FTIR) indicated changes in the bonding environment after activation, but did not identify a specific reaction product or a new dominant crystalline phase. Within the defined material-input boundary, SW replacement reduced NP consumption and the material-based carbon indicator, with the lowest carbon intensity per unit compressive strength (0.0113 kg CO2-eq./MPa) obtained for SW30-7.5M. The overall performance of the investigated AAMs depended on the combined effects of SW replacement level and NaOH concentration.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Experimental Study on the Influence of Waste Stone Powder on the Properties of Alkali-Activated Slag/Metakaolin Cementitious MaterialsCrystals · 2025
- Synergistic Impact of Bio-Based and Waste-Derived Contents on the Mechanical and Thermal Performance of Alkali-Activated Slag Mortars.Polymers · 2026
- Carbonation Curing and Mechanical Properties of Alkali-Activated Composites Derived from Calcined Granite Waste and Waste Ceramic PowderBuildings · 2026
- Influence of Expanded Polystyrene on the Mechanical and Tribological Performance of Alkali-Activated Lignocellulosic Ash Composites.Materials (Basel, Switzerland) · 2026
- Synergistic enhancement of mechanical, thermal, and durability properties in expanded perlite‐based lightweight alkali‐activated composites with basalt fiber and natural zeoliteStructural Concrete · 2025
- Evaluation of mineral waste streams for alkali-activated materials: Reactivity and utilization potentialJournal of Building Engineering · 2025