Selective Adsorption of Uranium from High Acid and High Chloride Zirconium Leach Liquor

Zhiping Yang, Haisheng Hu, Xiumin Jia, Absai Vatuva

Key points

From the paper's conclusion
  • These results support a process route integrating direct adsorption, selective iron stripping, and water elution, which enriches uranium into a concentrated eluate from industrial zirconium leach liquor.

Abstract

Uranium associated with zircon sand enters zirconium leach liquor during acid leaching and can subsequently migrate into downstream process streams. Its direct recovery from industrial leach liquor is challenging because of the high acidity, chloride concentration, and low U/Fe ratio. Here, a macroporous chelating anion-exchange resin (CU600) was evaluated for direct uranium recovery without neutralization, dilution, or Fe pre-reduction. CU600 achieved a batch uranium adsorption capacity of 7.5 g U/L wet resin and a removal efficiency of 42.3%, approximately 2.1 times those of D201. Laboratory dynamic loadings were 21.2 and 18.6 g U/L wet resin, while the on-site loading reached 20.9 g U/L wet resin. Despite feed U/Fe mass ratios of approximately 0.1, the loaded-resin U/Fe ratio exceeded 0.8. Reductive iron stripping removed 42.8% of co-loaded Fe with 6.8% U loss, increasing the resin-phase U/Fe ratio from 0.879 to 1.43. Subsequent water elution produced peak uranium concentrations of 30.4 g/L in the laboratory and 17.5 g/L on site. These results support a process route integrating direct adsorption, selective iron stripping, and water elution, which enriches uranium into a concentrated eluate from industrial zirconium leach liquor.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers