From the paper's conclusion
  • This value exceeded the practical benchmark pressure of 8 MPa used in the VSI standard, suggesting that the addition of boehmite nanofibers contributed to improving the mechanical strength of hollow spherical HAp particles.

Abstract

Hollow spherical hydroxyapatite (HAp) particles have potential as functional fillers and microcapsules; however, their low mechanical strength caused by their structural fragility limits their use. In this study, high-aspect-ratio boehmite nanofibers were incorporated into hollow spherical HAp particles by spray drying to improve their mechanical strength. A boehmite sol was added to an HAp aqueous solution prepared by the CO2 blowing method, and the mixed solution was spray-dried at 100 °C. Hollow spherical particles with a particle size of approximately 1 μm were obtained at boehmite sol additions up to 0.05 mass%. At 0.10 mass% addition, nozzle clogging and irregularly shaped particles were observed. Transmission electron microscopy observations showed fibrous structures within the hollow walls of the boehmite-containing particles. The average compressive strength increased from approximately 0.6 MPa without boehmite addition to approximately 8.5 MPa at 0.05 mass% addition. This value exceeded the practical benchmark pressure of 8 MPa used in the VSI standard, suggesting that the addition of boehmite nanofibers contributed to improving the mechanical strength of hollow spherical HAp particles.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers