Hybrid Modification of Bitumen with Waste Crumb Rubber, Polyethylene, and Vegetable Oil: Physical and Rheological Performance
Yunus Erkuş
Key points
From the paper's conclusion- The present investigation evaluates the potential of using waste crumb rubber (CR), polyethylene (PE) and vegetable oil (VO) in bitumen modification.
Abstract
Bitumen is markedly influenced by increasing traffic loads together with thermal conditions, so it is modified with various additives. One of the most frequently employed additives is Styrene-Butadiene-Styrene (SBS), but alternative additives, particularly those derived from waste, continue to be investigated because of concerns related to phase separation, cost, and sustainability. The present investigation evaluates the potential of using waste crumb rubber (CR), polyethylene (PE) and vegetable oil (VO) in bitumen modification. The physical and rheological characteristics of the bituminous binders were evaluated using softening point, penetration, rotational viscosity, storage stability, bending beam rheometer, and dynamic shear rheometer tests. CR + PE + VO modified binders are benchmarked against SBS-modified binders from performance and economic perspectives. Adding VO to PE+CR-modified binders reduces viscosity and makes the bitumen workable. PE produced the largest improvement in resistance against deformation at elevated temperatures, whereas VO provided the largest improvement in resistance against thermal cracking. The binder 333 (3% CR + 3% PE + 3% VO) exhibited more advantageous physical and rheological attributes relative to the binder modified with 4SBS (4% SBS). Master curves of complex viscosity were constructed according to the time–temperature superposition principle (TTSP) and subsequently fitted using the Cross and Carreau–Yasuda models. Both models closely reproduced the experimental data, with goodness-of-fit values exceeding 0.95. Among the evaluated binders, the 333 formulation exhibited the greatest zero-shear viscosity together with the lowest critical shear rate. This combination offers an estimated decrease in raw-material cost of roughly 20% compared with the 4SBS binder. Under the simplified material-cost/performance indices adopted in this study, the 333 exhibited roughly double the normalized index of the 4SBS formulation.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Preparation Optimization, Rheological Performance and Mechanism of High-Density Polyethylene and Crumb Rubber Composite-Modified Asphalt.Materials (Basel, Switzerland) · 2026
- Study on the Rheological Properties of Aged SBS-Modified Asphalt Rejuvenated with Soybean Oil and Crumb Rubber.Materials (Basel, Switzerland) · 2026
- Comparative performance evaluation of asphalt binder modified with high-content pretreated crumb rubber and various additivesJournal of Road Engineering · 2026
- Evaluation of binder and mixture performance in crumb rubber asphalt modified with SasobitConstruction and Building Materials · 2026
- Performance and Interaction Mechanisms of Bitumen Modified with Devulcanized Rubber-Recycled Polymer Composites.Polymers · 2026
- Rheological and Morphological Characterization of Asphalt Cement Hybrid-Modified with Waste-Derived Cellulose Fibers and Crumb Rubber.Polymers · 2026