Octadecylsilane-Functionalized Fe3O4 Nanoparticles Enhance Shape Fixity but Restrict Thermally Activated Shape Recovery in Thermoplastic Polyurethane Composites
Abdiel Elias, Angel Anaya, F. I. Espinosa-Lagunes, Juan G. Sotelo, Gonzalo Pincheira-Orellana, Martin Sepulveda, Cecilia D. Treviño-Quintanilla
Key points
From the paper's conclusion- We attribute the higher fixity and lower recovery primarily to the loss of physical netpoints; a contribution from particle–matrix interactions is possible but could not be separated with the present data.
Abstract
Magnetite (Fe3O4) is often added to thermoplastic polyurethane (TPU) to fabricate thermally actuated shape memory parts, but the particles tend to agglomerate and interact poorly with the matrix. We prepared TPU composites with 10 wt% Fe3O4, either as received or coated with octadecyltrichlorosilane (ODTS), by tetrahydrofuran (THF) solution casting followed by micro-injection molding. Neat and THF-processed TPU were included as references so that the effects of solvent, filler and surface treatment could be separated. The 5% mass-loss temperature (T95%) was 314.2 °C for neat TPU and 309.7 °C for THF-processed TPU; bare Fe3O4 lowered it to 284.8 °C and ODTS-Fe3O4 to 292.3 °C. In differential scanning calorimetry (DSC), the ODTS composite kept the soft-segment glass transition at −21 °C, but its hard-segment crystallization and melting enthalpies fell by 72% and 74%. The stress at 150% strain (17.9–18.6 MPa) did not differ among formulations (ANOVA, p = 0.49), whereas bare Fe3O4 raised Young’s modulus from 0.106 to 0.125 GPa (p = 0.036). In angular shape memory tests with recovery triggered in an oven at 90 °C, the ODTS composite fixed the temporary shape best (shape fixity ratio/Rf = 91.9% against 86.4% for neat TPU) and recovered least after 240 s (11.0% against 47.1%). Across the four materials, recovery tracked the hard-domain melting enthalpy. We attribute the higher fixity and lower recovery primarily to the loss of physical netpoints; a contribution from particle–matrix interactions is possible but could not be separated with the present data. Magnetic actuation was not evaluated in this study. Silane treatments for magnetite-filled TPU should therefore be judged by their effect on hard-segment ordering as well as on dispersion.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Highly Ductile PETG / POE /Fe 3 O 4 Multi‐Responsive Shape‐Memory Polymer for 4D PrintingPolymer Engineering & Science · 2026
- A Facile Preparation of Segmented Thermoplastic Polyurethane With Octamethyl Polyhedral Oligomeric Silsesquioxane‐Based Thermoresponsive Programmable Shape Memory Nanocomposites With Enhanced Mechanical PerformanceSPE Polymers · 2026
- Tuning the Thermomechanical Performances of TPU ‐ POSS Composites Through Controlled Microstructural EvolutionPolymer Composites · 2026
- Influence of Heat Treatment on the Mechanical and Chromatic Properties of Polyetheretherketone‐ TiO 2 Composite Manufactured Using Fused Deposition ModelingJournal of Applied Polymer Science · 2026
- Surface Functionalization of Thermoplastic Polyurethane Scaffolds to Enhance Microparticle Attachment.ACS biomaterials science & engineering · 2026
- Experimental Investigation of Nanodiamond Reinforcement in PU for Enhancing Mechanical, Scratch, Rheological, Thermal, and Shape-Memory PropertiesPolymers · 2025