Polymers

Rigid–Flexible Synergy in Heterocyclic Siloxane-Tailored Poly(propylene carbonate)-Based Thermoplastic Polyurethane Elastomers

Bingru Li, Siyu Zhao, Shuanjin Wang, Min Xiao, Zhuofeng Ke, Yuezhong Meng

Key points

From the paper's conclusion
  • Poly(propylene carbonate) diol (PPCDL) can incorporate CO2 directly into the soft segment of a thermoplastic polyurethane (TPU); however, its rigid and strongly polar carbonate backbone suppresses microphase separation, so lower hardness is usually achieved only at the expense of tensile strength.

Abstract

Poly(propylene carbonate) diol (PPCDL) can incorporate CO2 directly into the soft segment of a thermoplastic polyurethane (TPU); however, its rigid and strongly polar carbonate backbone suppresses microphase separation, so lower hardness is usually achieved only at the expense of tensile strength. Herein, this trade-off was addressed by molecular design rather than formulation adjustment within this fixed formulation window. By utilizing a rigid–flexible synergetic strategy, six heterocyclic siloxane modifiers bearing triazole, thiadiazole, or aniline pendants, along with three amino-terminated poly(dimethylsiloxane) (PDMS) controls, were incorporated into PPCDL-based TPUs as chain-extending segments via a torque-rheometer-assisted bulk process at a fixed hard-segment content of 17 wt% and a [NCO]/[OH] ratio of 1.02. Each modifier couples a flexible siloxane spacer with heterocyclic hydrogen-bonding moieties, and the N–H donor and sp2-hybridized nitrogen acceptor counts were explicitly enumerated. The long-chain triazole modifier L2 afforded the most balanced elastomer, with a Shore A hardness of 76, a tensile strength of 5.71 ± 0.44 MPa, and an elongation at break of 892 ± 54%; these values exceeded those of the best PDMS control (4.36 ± 0.33 MPa, 621 ± 0.97%, 80 Shore A) in all evaluated metrics, without any petroleum-based polyol. Gaussian deconvolution of the N–H stretching band showed that the ordered hydrogen-bonded fraction, rather than the total N–H content, correlated with tensile strength (r = 0.723) and hardness (r = 0.732). Because all formulations share a 17 wt% hard segment, R = 1.02, a single PPCDL molar mass, and a single heterocyclic modifier loading, the proposed design rules should be regarded as qualitative guidelines whose transferability remains to be validated.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers

Rigid–Flexible Synergy in Heterocyclic Siloxane-Tailored Poly(propylene carbonate)-Based Thermoplastic Polyurethane Elastomers — Science Skim