Polymers

Sequential Dual-Cure Thiol-Epoxy Vitrimer Nanocomposites from Click Chemistry: Advanced Properties and Multifunctionality.

Ignacio Collado, Antonio Vázquez-López, Alberto Jiménez-Suárez, Silvia G Prolongo

Materials Science and Engineering Area, Escuela Superior de Ciencias Experimentales y Tecnología, Universidad Rey Juan Carlos, C/Tulipán s/n, 28933 Móstoles, Madrid, Spain.

Key points

From the paper's conclusion
  • Activation energies were 74–89 kJ mol−1; Arrhenius extrapolation predicted mean relaxation times of 30 min at 184–195 °C, below the reported 225 °C stability limit.

Abstract

Sequential dual curing enables staged shaping of multifunctional thermosets. DGEBA/thiol/1-methylimidazole composites containing multi-walled carbon nanotubes (MWCNT), graphene nanoplatelets (GNP), Fe3O4 or Fe2O3 were assessed for curing, morphology, thermomechanical properties, electrical and thermal transport, self-heating, shape memory, de-icing, shielding, strain sensitivity, wettability, storage stability and stress relaxation. Carbon fillers (thiol:epoxy ratio r = 0.7) and oxides (r = 0.8) used matching unfilled controls and volume-fraction normalisation. MWCNT enabled electrical actuation and in situ curing, with a model-free percolation bracket of 0.003-0.006 vol % and 18.6 dB shielding at 0.10 vol %. GNP favoured thermal management and electrothermal de-icing: thermal conductivity rose from 0.20 to 1.25 W m-1 K-1, the critical Joule field fell below 1 V mm-1 and the average-to-maximum overheat ratio reached 0.9. GNP also achieved 24 dB shielding. Fe3O4 favoured thermomechanical reinforcement, raising Tg by 13.6 K at 1.2 vol %; shape fixity reached 99.7%. Fe2O3 favoured contactless heating, reaching a 100 K average overheat at 85-165 mT. Representative formulations showed stress relaxation consistent with bond exchange, with filler-induced changes in mean relaxation time at 180 °C within a factor of 1.5. Activation energies were 74-89 kJ mol-1; Arrhenius extrapolation predicted mean relaxation times of 30 min at 184-195 °C, below the reported 225 °C stability limit. Filler selection must preserve the second cure.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers