Pulsed Electromagnetic Field-Stimulated Alginate-Chitosan/Hydroxyapatite Nanocomposite Scaffolds for Accelerated Repair of Critical-Size Femoral Bone Defects.

Ahmed Abd El-Fattah, Safa O Emara, Khaled O Sebakhy, Mustapha El Hariri El Nokab, Ahmed M El-Khatib, Sherif H Kandil, Alaa M Khalil

Department of Materials Science, Institute of Graduate Studies and Research, Alexandria University, El-Shatby, Alexandria 21526, Egypt. · Department of Chemical Engineering, School of Engineering (EDICT), Bahrain Polytechnic, Isa Town P.O. Box 33349, Bahrain.

Key points

From the paper's conclusion
  • Together, they suggest that coupling an Alg-CS/HA nanocomposite scaffold with low-frequency, high-intensity PEMF stimulation is a promising, non-invasive strategy for enhancing the repair of critical-size bone defects, warranting confirmation in larger studies.

Abstract

Critical-size bone defects remain a major clinical challenge, as impaired endogenous healing and an unfavorable local microenvironment prevent spontaneous bridging of the defect. Here, we report a bio-physical regenerative strategy that combines a three-dimensional, porous alginate-chitosan/hydroxyapatite (Alg-CS/HA) nanocomposite scaffold with targeted pulsed electromagnetic field (PEMF) stimulation. Rod-like hydroxyapatite (HA) nanoparticles (~12 × 86 nm, Ca/P = 1.64) were synthesized and incorporated at 30 wt% into an ionically crosslinked Alg-CS polyelectrolyte matrix. HA incorporation significantly increased the compressive strength (22.41 ± 1.35 vs. 14.53 ± 1.81 kPa) and modulus (156.51 ± 2.15 vs. 74.34 ± 1.43 kPa) of the scaffold, while preserving an interconnected porous architecture (75.97 ± 7.8% porosity) and slowing enzymatic biodegradation (76.70 ± 3.82% mass loss at 28 days). MTT assays on human skin fibroblasts confirmed that both formulations were highly cytocompatible, with viability exceeding 85% at concentrations up to 50 mg/mL. In vivo, bilateral critical-size femoral defects (6 mm diameter) were created in New Zealand rabbits to evaluate bone regeneration under two PEMF regimes (5 and 50 Hz; 0.22 and 0.5 mT) applied for 3 weeks. Untreated defects showed essentially no repair (1.0 ± 2.4%), whereas scaffold implantation alone yielded 20.0 ± 4.3% new bone formation. PEMF stimulation produced a clear frequency- and intensity-dependent enhancement of osteogenesis, culminating in 90.0 ± 5.2% defect bridging in the low-frequency, high-intensity group (5 Hz, 0.5 mT), a 4.5-fold increase over the scaffold-only control. Histological analysis showed dense, mature trabecular bone with abundant osteocytes, active osteoid deposition, and histological features consistent with vascularization in this group. These preliminary results were obtained with n = 3 defect sites per group. Together, they suggest that coupling an Alg-CS/HA nanocomposite scaffold with low-frequency, high-intensity PEMF stimulation is a promising, non-invasive strategy for enhancing the repair of critical-size bone defects, warranting confirmation in larger studies.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers

Pulsed Electromagnetic Field-Stimulated Alginate-Chitosan/Hydroxyapatite Nanocomposite Scaffolds for Accelerated Repair of Critical-Size Femoral Bone Defects — Science Skim