Solid-State Sulfonation of Dense Poly(2,6-Dimethyl-1,4-Phenylene Oxide) Films: Membrane Properties and Electrochemical Assessment at MEA Level.
Carlo De Luca, Emmanuel De Gregorio, Martina Butori, Björn Eriksson, Rakel W Lindström, Viviana Cigolotti, Elio Jannelli, Claudio Ferone,
Department of Chemical Sciences, University of Naples Federico II, Complesso Universitario di Monte Sant'Angelo, Via Cintia, 80126 Napoli, Italy. · Department of Engineering, University of Naples 'Parthenope', Centro Direzionale, Isola C4, 80143 Napoli, Italy.
Key points
From the paper's conclusion- Together with swelling, tensile, and Fenton data, these results identify dimensional control, oxidative stabilization, and better membrane–ionomer compatibility as the next steps and provide a quantitative MEA-level baseline for solid-state sulfonated PPO membranes.
Abstract
Fluorine-free hydrocarbon proton-exchange membranes offer an alternative to perfluorosulfonic acid (PFSA) electrolytes, but good membrane-level properties do not always translate into membrane-electrode assembly (MEA) performance. Here, dense poly(2,6-dimethyl-1,4-phenylene oxide) (PPO) films were sulfonated in the solid state, yielding a sulfur distribution that appeared homogeneous through the membrane thickness and ion-exchange capacities (IEC) of 1.17-2.20 meq g-1, corresponding to sulfonation degrees of 16-32 mol% and water uptake from 55 to 92%. The sulfonated PPO (sPPO) membrane with the highest IEC that remained self-standing was tested in a single-cell MEA and compared with a Nafion® 212-based MEA prepared and operated in the same way. The sPPO-based MEA showed lower hydrogen crossover and higher apparent short-circuit resistance than the Nafion® 212 reference. However, its high-frequency resistance (HFR) was also higher, corresponding to an apparent MEA-level conductivity of 11 mS cm-1 at 80 °C and 70% RH, compared with 40 mS cm-1 for Nafion® 212. This gap persists even though sPPO has a higher hydration number. Since the catalyst layers contain a PFSA ionomer, this HFR-based conductivity includes membrane, electrode, and interfacial contributions. The sPPO membrane reached a peak power density of 0.45 W cm-2 at 80 °C and 90% RH. In a short-term potentiostatic test, the sPPO-based MEA failed after approximately 6 h. Together with swelling, tensile, and Fenton data, these results identify dimensional control, oxidative stabilization, and better membrane-ionomer compatibility as the next steps and provide a quantitative MEA-level baseline for solid-state sulfonated PPO membranes.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Sulfonated polybenzimidazole for low-alkalinity ion solvating membrane water electrolysisNature Energy · 2025
- Dimensionally Stable Cross-Linked Hydroxyl-Functionalized Sulfonated Poly(ether ether ketone) with Low H2 Crossover and High Proton Conductivity for High-Performance H2 Sensing.ACS sensors · 2026
- Effects of PFSA Ionomer Side-Chain Structure on PEMFC Performance and Transport Properties Under Near-Boiling-Point ConditionsEnergies · 2026
- Balanced Ionic Conductivity and Permselectivity of Cation Exchange Membranes Prepared from Sulfonated Poly(ether sulfone)ACS Omega · 2025
- Advances in Performance Degradation Mechanisms and Improvement Measures of Perfluorosulfonic Acid Ionomers in Catalyst Layers of Proton Exchange Membrane Fuel Cells Under Moderate‐Temperature and Low Relative Humidity Operation: A ReviewAdvanced Energy Materials · 2026
- Fluorine-Substituent-Containing Sulfonated Poly(arylene ether) Membranes with Enhanced Proton Conductivity and Dimensional Stability for Proton Exchange Membrane Fuel Cells.Molecules (Basel, Switzerland) · 2026