Effect of AKD Content on Wettability, Water Absorption Kinetics, and Interfacial Properties of Poplar Wood Flour/PLA Biocomposites.
Jiahui Zhang, Xiao Wu, Shengze Gong, Xia Yang, Hongbo Li, Zebing Xing, Yu Xian
The College of Forestry, Shanxi Agricultural University, Jinzhong 030801, China. · The College of Agricultural Engineering, Shanxi Agricultural University, Jinzhong 030801, China.
Key points
From the paper's conclusion- These findings support the water-resistant modification of PLA-based wood–plastic composites.
Abstract
In this study, poplar wood flour was modified with alkyl ketene dimer (AKD), and poplar wood flour/polylactic acid (PLA) composites with 0-5% AKD were prepared. Effects of AKD content on wettability, water absorption kinetics, dimensional stability, flexural properties, and microscopic interface were investigated. AKD likely consumed hydroxyl groups through esterification and/or hydrogen bonding, as reported in the literature, and introduced hydrophobic alkyl chains. The 5% AKD sample exhibited the highest contact angle, while the 3% AKD sample showed the lowest total surface free energy (24.73 mJ·m-2). AKD content significantly changed the water diffusion mode: at 0-3% AKD, water absorption followed non-Fickian diffusion, with 2% AKD showing the highest n value (0.7132), indicating swelling-controlled diffusion and the lowest apparent saturation water absorption. At 4% AKD, n decreased to 0.4786, approaching Fickian diffusion, and agglomerated pores accelerated water transport. The 2% AKD sample exhibited optimal interfacial bonding and the highest flexural strength retention (46.29%). The 5% AKD sample showed the lowest steady-state thickness swelling coefficient (10.03%), indicating the best dimensional stability, but agglomeration defects weakened mechanical properties. Interfacial bonding strength, rather than low water absorption or low swelling, was key to mechanical retention. An optimal AKD content range exists when "optimal" is defined by the balance between mechanical retention and dimensional stability: 2% AKD is preferred for mechanical retention, while 5% AKD is preferred for dimensional stability under humid service scenarios. These findings support the water-resistant modification of PLA-based wood-plastic composites.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Regulation of bonding performance in cellulose-based adhesive and adhesive film via wood surface activationColloids and Surfaces A Physicochemical and Engineering Aspects · 2026
- Aldehyde-enabled interfacial engineering of lignocellulosic nanofibrils and wood surfaces for reliable bio-based wood bonding.International journal of biological macromolecules · 2026
- Bio-based adhesives from distillers’ dried grains and soybean for wood composites:review on performance and sustainabilityEuropean Journal of Wood and Wood Products · 2026
- Effect of PLA-g-MAH Content on the Interfacial Structure and Properties of Wheat Straw/PLA Biocomposites.Polymers · 2026
- Poly(itaconic acid)-functionalized kraft lignin (PIA-f-Lig) and chitosan derived fully biocomposite with enhanced water resistance, mechanical strength, wet wood adhesion, and antioxidant activityColloids and Surfaces B Biointerfaces · 2026
- Bamboo particleboards bonded with lignin-modified vinyl acetate-ethylene adhesive: physical, mechanical, and thermal propertiesEuropean Journal of Wood and Wood Products · 2026