Comparative Evaluation of Hydrofluoric Acid Etchants on a 3D-Printed Lithium Disilicate-Filled Polymer Resin.
Silvia Rojas-Rueda, Fabio Luiz Andretti, Carlos A Jurado, Rene Garcia-Contreras, Jose Vivaldi, Abdullah Almansour, Hamad Algamaiah, Abdulrahman Alshabib
School of Dental Medicine, Ponce Health Sciences University, Ponce 00716, Puerto Rico. · Division of Operative Dentistry, Department of General Dentistry, College of Dentistry, University of Tennessee Health Science Center, Memphis, TN 38103, USA.
Key points
From the paper's conclusion- These findings characterize surface modification of a 3D-printed lithium disilicate-filled polymer resin and should not be generalized to conventional lithium disilicate ceramics.
Abstract
BACKGROUND: This in vitro study compared the effects of four commercial hydrofluoric acid etchants with different nominal concentrations on the surface roughness of a 3D-printed lithium disilicate-filled polymer resin, evaluated after post-polymerization without debinding or sintering. METHODS: Seventy-five specimens were randomly assigned to five groups (n = 15): G1, 4.5% hydrofluoric acid (IPS Ceramic Etching Gel, Ivoclar); G2, 4% hydrofluoric acid (Porcelain Etchant, Bisco); G3, 9.5% hydrofluoric acid (Porcelain Etchant, Bisco); G4, 9% hydrofluoric acid (Porcelain Etch, Ultradent); and G5, an unetched control. Etchants were applied for 20 s. Areal surface roughness (Sa) was measured using non-contact optical profilometry. Data were analyzed using Levene's test, conventional and Welch's analyses of variance, and Games-Howell pairwise comparisons (α = 0.05). RESULTS: Both analyses of variance identified significant differences among groups (p < 0.001). All pairwise comparisons were statistically significant (p < 0.001). Mean Sa values were 0.1558 ± 0.0159 µm for G5, 0.3159 ± 0.0313 µm for G1, 0.5093 ± 0.0467 µm for G2, 0.7243 ± 0.0409 µm for G3, and 0.9365 ± 0.0408 µm for G4. The 9% Ultradent etchant produced the greatest roughness, approximately six times the control value. CONCLUSIONS: All etchants significantly increased surface roughness. However, the ranking did not follow nominal acid concentration, and differences in commercial formulations prevent attribution of the observed effects to concentration alone. These findings characterize surface modification of a 3D-printed lithium disilicate-filled polymer resin and should not be generalized to conventional lithium disilicate ceramics. Further studies are needed to determine whether these topographic changes improve subsequent adhesive bond strength or long-term durability.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Influence of Polishing Treatment on the Topography of 3D-Printed Provisional Resins: An In Vitro Study.International journal of dentistry · 2026
- Effect of pH and Temperature on the Surface Roughness of 3D-Printed and Milled Dental Hybrid Resin–CeramicPolymers · 2025
- Comparative Evaluation of Novel and Conventional Acid Etchants on the Surface Roughness of Lithium Disilicate and Zirconia Ceramics.International journal of dentistry · 2026
- Effects of different polishing systems on the surface roughness, microhardness and gloss of 3D-printed resinsBMC Oral Health · 2025
- Combined Effects of Print Orientation and Post-Curing Duration on the Mechanical and Surface Properties of a 3D-Printable Resin Intended for Lingual Retainers: An In Vitro Study.Polymers · 2026
- Effect of denture cleansing solutions on physical properties of 3D-printed and heat-polymerized denture base resinsBMC Oral Health · 2026