A Phosphorus-Containing Polyamide Oligomer as a Synergist for Flame-Retardant PA66/GF Composites: Concurrent Improvements in Flame Retardancy and Electrical Safety.
Xing Zhang, Lirong Xie, Zhongliang Zhang, Guanghao Guo, Zhichao Zhen, Xuran Liu, Dan Huang
College of Materials Engineering, North China Institute of Aerospace Engineering, Langfang 065000, China. · National Engineering Research Center of Engineering and Ecological Plastics, Technical Institute of Physics and Chemistry, Chinese Academy of Sciences, Beijing 100190, China.
Key points
From the paper's conclusion- Compared with the conventional 20-part system, total additive loading decreased by 30%, with simultaneous improvements in flame retardancy, electrical safety, and mechanical properties.
Abstract
As electronics become smaller and more power-dense, glass-fiber-reinforced polyamide 66 (PA66/GF) must combine halogen-free flame retardancy with electrical safety, including a glow-wire ignition temperature (GWIT) ≥ 775 °C and a comparative tracking index (CTI) ≥ 600 V. Conventional low-molecular-weight flame retardants often require loadings above 15 parts by mass, impairing mechanical and electrical properties. Here, a phosphorus-containing polyamide oligomer (DOPO-MA-oligomerPA6) was synthesized via a DOPO-MAH intermediate from 9,10-dihydro-9-oxa-10-phosphaphenanthrene-10-oxide (DOPO) and maleic anhydride (MAH), followed by polymerization with ε-caprolactam, then melt-blended with aluminum diethylphosphinate (ADP) and melamine polyphosphate (MPP) in PA66/GF. Its oligo-PA6 backbone provides good compatibility with PA66, while its low molecular weight (Mn = 10,984 g mol-1; PDI = 2.569) favors dispersion. The phosphorus groups enhance the efficiency of the ADP/MPP system. With 4 parts oligomer and a total flame-retardant loading of 14 parts by mass per 100 parts PA66/GF, the composite achieved UL-94 V-0 rating, a limiting oxygen index (LOI) of 36.1%, a GWIT of 800 °C, and a CTI of 600 V. Its heat deflection temperature, tensile strength, notched impact strength, and flexural modulus were 178.8 °C, 95.0 MPa, 8.7 kJ m-2, and 8984 MPa, respectively. Compared with the conventional 20-part system, total additive loading decreased by 30%, with simultaneous improvements in flame retardancy, electrical safety, and mechanical properties. This offers a scalable route to high-performance PA66/GF composites.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Flame‐Retardant Performance of PA6 Modified by Amide‐Based Cyclophosphazene Derivative Combined With Aluminum DiethylphosphinateJournal of Applied Polymer Science · 2026
- Synthesis of Polyamide 66 Copolymers with Inherent Flame Retardancy and Enhanced Mechanical PropertiesACS Applied Polymer Materials · 2026
- Glycidyl ether-terminated branched polysiloxane and its synergy with DOPO for the preparation of flame-retardant, high-strength, and high-toughness epoxy resinResults in Engineering · 2025
- Effects of Interfacial Compatibility on Synergistically Improving the Flame Retardancy and Mechanical Properties of PA6 CompositesPolymer Composites · 2026
- Synergistic modification of long-chain polyamides with brominated polystyrene/Sb 2 O 3 for high-performance flame-retardant PA66 compositesInternational Polymer Processing · 2026
- Achieving High Toughness Retention and Flame Retardancy in PC / ABS Alloys by the Synergistic AHP / DSPSi System With Reactive CompatibilizationJournal of Applied Polymer Science · 2026