Organic-Acid-Modified and PCE-Hybrid Grinding Aids in Slag-Blended Cements: Linking Particle Size Distribution to Hydration and Strength.
Veysel Kobya, Yahya Kaya, Ali Mardani
Department of Civil Engineering, Faculty of Engineering, Bursa Uludag University, Bursa 16059, Turkey.
Key points
From the paper's conclusion- Overall, grinding-aid selection should consider particle-size distribution, hydration, BFS characteristics, and replacement level, rather than relying on Blaine fineness alone, and should also account for additive chemistry and the potential influence of polymer-containing formulations on the interfacial properties of ground cement particles.
Abstract
Reducing clinker content while maintaining the performance of slag-blended cement requires grinding-aid strategies that improve grinding efficiency and support subsequent hydration. In this study, commercial triisopropanolamine (TIPA), diethanolisopropanolamine (DEIPA), and diethylene glycol (DEG), their organic-acid-modified derivatives, and their hybrids with a polycarboxylate ether (PCE)-based grinding aid were evaluated at 0.05% in cement systems containing two granulated blast-furnace slags (BFSs) with different physical and chemical characteristics. Particle-size distribution, X-ray diffraction, thermogravimetric analysis, scanning electron microscopy, zeta potential, PCE adsorption, and compressive strength tests were used to investigate the relationships between grinding-aid chemistry, particle characteristics, hydration, and mechanical performance. Similar Blaine fineness values did not necessarily yield comparable particle-size distributions or hydration responses, indicating that Blaine fineness alone is insufficient to assess the effectiveness of grinding aids in BFS-blended cement. Organic-acid modification was generally more effective than PCE hybridization, depending on the original grinding-aid chemistry. M-TIPA promoted the strongest hydration development and the highest 28- and 56-day strengths at all BFS replacement levels. At 30% replacement, M-TIPA mixtures with BFS 1 and BFS 2 reached 28-day strengths of 45.82 and 46.55 MPa and 56-day strengths of 52.69 and 54.13 MPa, respectively, exceeding the clinker-only control. At 45% replacement, modified alkanolamines reduced, but did not eliminate, strength loss, whereas clinker dilution dominated at 60%. Overall, grinding-aid selection should consider particle-size distribution, hydration, BFS characteristics, and replacement level, rather than relying on Blaine fineness alone, and should also account for additive chemistry and the potential influence of polymer-containing formulations on the interfacial properties of ground cement particles.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Sustainable Cement Production: TEA-TIPA as Grinding Aids: Optimizing Ratios for Efficiency and Environmental ImpactPolymers · 2025
- Hydration, mechanical, and environmental performance of blended cements incorporating ground granulated blast furnace slag, ground waste bottle glass, and metakaolinFrontiers in Materials · 2026
- Particle-Size-Fractionated Coal Gasification Slag as a Supplementary Cementitious Material: Hydration Products, Microstructure Evolution, and Mechanical Performance via Classified Grinding.Materials (Basel, Switzerland) · 2026
- Hydration and microstructure of ternary slag cements incorporating recycled concrete finesConstruction and Building Materials · 2026
- Usage of BOF Slag and Next Generation EAF Slag in the Cement IndustryJournal of Sustainable Metallurgy · 2026
- Mineral reconstruction of high-volume phosphogypsum driven by a slag-based composite stabilizer: mechanisms of subgrade performance enhancement and phosphorus/fluoride immobilization.Journal of hazardous materials · 2026