Comparative Impact Response, Damage, and Healing Performance of CFRP Laminates with Different Thicknesses and Reinforcement Architectures.
Maryna Shevtsova, Valentin Rougier, Véronique Michaud, Oleksii Vambol, Svitlana Purhina
Laboratory of Composite Materials, Vilnius Gediminas Technical University, 10223 Vilnius, Lithuania. · Laboratory for Processing of Advanced Composites, École Polytechnique Fédérale de Lausanne, 1015 Lausanne, Switzerland.
Key points
From the paper's conclusion- Overall, the investigated laminate configurations exhibited distinct impact responses, internal damage patterns, residual strengths, and levels of mechanical recovery after healing.
Abstract
Carbon-fiber-reinforced polymer (CFRP) laminates can exhibit different low-velocity impact responses and post-impact performance depending on laminate configuration. This study compares three self-healing CFRP configurations manufactured from CompPair HealTech® materials: 1.45 and 3.30 mm unidirectional (UD) laminates and a 2.66 mm woven laminate. Low-velocity impact tests were performed at 5 and 10 J. Internal damage was qualitatively examined using visual inspection and X-ray phase-contrast imaging (XPCI), while post-impact performance and recovery were assessed by compression-after-impact (CAI) testing before and after thermal healing. The 1.45 mm UD laminate exhibited the largest displacement and lowest maximum impact force, whereas the 3.30 mm UD laminate showed the highest force and smallest displacement, with the woven laminate exhibiting an intermediate response. Despite its greater impact stiffness, the 3.30 mm UD laminate showed the largest relative reduction in residual compressive strength after 10 J, with strength retention decreasing from approximately 98% after 5 J to 64% after 10 J. The 1.45 mm UD and woven laminates retained 89% and 88% after 5 J and 82% and 72% after 10 J, respectively. After healing, the 1.45 mm UD and woven laminates recovered to approximately 99% of their virgin strengths after 5 J. After 10 J, strength retention reached 91%, 79%, and 81% for the 1.45 mm UD, 3.30 mm UD, and woven laminates, with corresponding healing efficiencies of 49%, 42%, and 31%, respectively. XPCI revealed configuration-dependent internal damage patterns that became more pronounced at 10 J. Overall, the investigated laminate configurations exhibited distinct impact responses, internal damage patterns, residual strengths, and levels of mechanical recovery after healing.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Influence of Resin Content on the Low‐Velocity Impact Response and Compression‐After‐Impact Performance of Carbon Fiber/Epoxy LaminatesInternational Journal of Polymer Science · 2026
- Low-Velocity Impact Damage and Residual Tensile Performance of CFRP Plates with Embedded Steel WiresBuildings · 2026
- Effect of Curvature Height on the Low-Velocity Impact Behaviour of Unidirectional T300/5208 CFRP Laminated Shell Panels: A Comparative Numerical Parametric Analysis of Intralaminar + Interlaminar and Intralaminar-Only ModelsPolymers · 2026
- Low-Velocity Impact Response of Small-Scale RC Beams Strengthened with CFRP: Experimental and Numerical InvestigationApplied Sciences · 2026
- The Behavior of Beams Reinforced with Patches Under Three-Point Bending: An Experimental InvestigationPolymers · 2025
- Residual Tensile Strength of CFRP Panels with Dual Stepped-Lap Repairs: Effects of Ligament Spacing, Patch Lay-Up, and Repair Arrangement.Polymers · 2026